MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Parker Chomerics Tecknit® 72-08116 Silver-Filled Epoxy System
Categories: Polymer; Thermoset; Epoxy; Epoxy Cure Resin

Material Notes: Description: This is a silver filled epoxy system designed for maximum performance and lowest volume resistivity. It is easily mixed 1:1 by volume or weight, from the two one-ounce jars. Its consistency is that of a thick paste, making it easy to dispense and apply.

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Shear Strength >= 9.65 MPa>= 1400 psiCured; ASTM D1002
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 0.0010 ohm-cm<= 0.0010 ohm-cmCured; QAP-1017
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 149 °C300 °FCured
Minimum Service Temperature, Air -62.0 °C-79.6 °FCured
Shrinkage <= 1.0 %<= 1.0 %Cured
 
Processing PropertiesMetricEnglishComments
Cure Time  30.0 min
@Temperature 100 °C
0.500 hour
@Temperature 212 °F
Recommended Cure
 30.0 min
@Temperature 100 °C
0.500 hour
@Temperature 212 °F
Followed by 24 hrs @ RT
Pot Life 45 min
@Temperature 25.0 °C
45 min
@Temperature 77.0 °F
Shelf Life 15.0 Month15.0 MonthUnopened Container
 
Descriptive Properties
ColorBright Silver
ConsistencyThick Paste
FillerAg
Final ConditionRigid
Mix Ratio1:1
Number of ComponentsTwo
ResinEpoxy
Volume1.5 in3
Weight2 oz

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHOME409 / 131119

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.