MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Geon® Performance Solutions 87725 Sheet PVC  (discontinued **)
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Sheet Grade

Material Notes: Exterior, Low Gloss. Exterior grade, impact modified, rigid PVC sheet compound designed for low gloss sheet applications that require thermoformability.

Data provided by the manufacturer, The Geon Company.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.44 g/cc0.0520 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8282ASTM D2240
Tensile Strength, Ultimate 46.0 MPa6670 psiat 5 cm/min. ASTM D638
Modulus of Elasticity 2.554 GPa370.4 ksiat 5 cm/min. ASTM D638
Flexural Yield Strength 83.0 MPa12000 psiASTM D790
Flexural Modulus 2.901 GPa420.8 ksiASTM D790
Izod Impact, Notched 3.50 J/cm
@Diameter 3.20 mm
6.56 ft-lb/in
@Diameter 0.126 in
bars; ASTM D256
 
Thermal PropertiesMetricEnglishComments
CTE, linear 63.1 µm/m-°C
@Temperature 20.0 °C
35.1 µin/in-°F
@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 66.0 °C151 °FUnannealed; 6.4 cm (2.5 in.) bars; ASTM D648
 
Processing PropertiesMetricEnglishComments
Melt Temperature 199 - 210 °C390 - 410 °FExtrusion

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CoreLite PVC 48 Closed-Cell PVC Foam Sheet
Overview of materials for PVC, Sheet Grade
Pearl Engineering PEPLPET B-101C PET Sheet Grade
Armacell Ensolite™ 1400 Continuous Rolls/Sheets
Geon® Performance Solutions 87655 Sheet PVC

PVIGF8 / 71893

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.