MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Aluminum Titanium Nitride (AlTiN) PVD Coating
Categories: Ceramic; Nitride; Other Engineering Material; Ceramic/Metallic Coating

Material Notes: Also called Titanium Aluminum Nitride (TiAlN); it is a complex structure consisting of TiN and AlN bonds in a crystalline matrix. This black colored coating is a high performance coating which is good at machining of abrasive and difficult-to-machine materials such as cast iron, aluminum alloys, tool steels, and nickel alloys. TiAlN offers improved ductility that makes it an outstanding choice for interrupted cutting operations, while its superior oxidation resistance provides good performance in high temperature machining. Typical coating thickness is 1-5 µm. Adhesion measured by scratch test is 70/80 N. Lower friction and higher hardness than TiAlN.

Data provided by BryCoat Inc.

Key Words: Hard Ceramic Coatings; Brycoat; Aerospace Coatings
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Knoop Microhardness 40004000HK 25 (25 gf load)
Coefficient of Friction 0.450.45between 100 Cr6 ball and coating
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 788 °C1450 °FOxidation Begins
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Titanium Aluminum Nitride (TiAlN) PVD Coating
Titanium, Ti
Titanium Carbonitride (TiCN) PVD Coating
Titanium Nitride (TiN) Coating
Chromium Nitride (CrN) PVD Coating

BNTiA1 / 271

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.