MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Saint-Gobain COHRlastic® TC100U Uncured Thermally Conductive Solid Silicone Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Silicone; Silicone Elastomer, for Thermal Management

Material Notes: COHRlastic® solid silicone rubber in square sheet and continuous length form has a smooth, blemish-free surface. It is available in degrees of hardness from relatively soft 30 Durometer to the relatively hard 70 Durometer on the Shore A scale. It is manufactured in different formulations to provide a choice of physical properties and cost considerations. TC100U, in the uncured state, is an effective system for bonding printed circuit boards, heat sinks and electronic components to a variety of substrates. Refrigerated storage is required. WHITE in color. All data based on a 0.0625 inch test sample.(Also comes in 1/32" thickness.)
Information provided by Saint Gobain Performance Products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6565
Elongation at Break 350 %350 %
Tear Strength 35.1 kN/m200 pli
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cm
Dielectric Strength 9.84 kV/mm250 kV/in
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 1.55 W/m-K10.7 BTU-in/hr-ft²-°F
 
Descriptive Properties
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Silicon Nitride
Silicon Nitride, Sialon
Silicon Nitride, reaction sintered
Silicon Nitride, RBSN
Silicon Nitride, HPSN

PSTGQZ244 / 68758

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.