MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Bakelite® UP 3620 Unsaturated Polyester Resin, High Surface Quality, UL Listed
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Polyester, TS; Thermoset Polyester Glass Filled BMC

Material Notes: Polyester molding compound, mainly organically filled, styrene free, processing shrinkage as for phenolic molding compounds, non flammable, high surface quality, UL listed molding compound 1,5 mm / V-0 (ALL).

Applications: Lamp parts, switch gears, housings and base plates, MCB housings.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.71 g/cc0.0618 lb/in³ISO 1183
Apparent Bulk Density 0.700 g/cc0.0253 lb/in³ISO 60
Linear Mold Shrinkage 0.0070 cm/cm0.0070 in/inCompression Molding. Post Shrinkage = 0.25%.; ISO 2577
 0.0075 cm/cm0.0075 in/inInjection Molding. Post Shrinkage = 0.25%.; ISO 2577
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 250 MPa36300 psiH961/30; ISO 2039/P1
Tensile Strength 50.0 MPa7250 psiISO 527 - 1/2
Tensile Modulus 8.50 GPa1230 ksiISO 527 - 1/2
Flexural Strength 80.0 MPa11600 psiISO 178
Flexural Modulus 7.50 GPa1090 ksiISO 178
Compressive Strength 180 MPa26100 psiISO 604
Charpy Impact Unnotched 0.750 J/cm²3.57 ft-lb/in²ISO 179-1 eU
Charpy Impact, Notched 0.190 J/cm²0.904 ft-lb/in²ISO 179-1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+12 ohm-cm1.00e+12 ohm-cm
Surface Resistance 1.00e+11 ohm1.00e+11 ohm
Dielectric Constant 5.0
@Frequency 100 Hz
5.0
@Frequency 100 Hz
Dielectric Strength 30.0 kV/mm
@Thickness 1.00 mm
762 kV/in
@Thickness 0.0394 in
IEC 60243-P1
Dissipation Factor 0.020
@Frequency 100 Hz
0.020
@Frequency 100 Hz
Arc Resistance 140 - 145 sec140 - 145 secASTM D495
High Voltage Arc Resistance to Ignition (HVAR) >= 300 sec
@Thickness 1.50 mm
>= 300 sec
@Thickness 0.0591 in
(ALL)
Comparative Tracking Index 600 V600 V
Hot Wire Ignition, HWI  60 - 120 sec
@Thickness 1.50 mm
60 - 120 sec
@Thickness 0.0591 in
(ALL)
 >= 120 sec
@Thickness 3.00 mm
>= 120 sec
@Thickness 0.118 in
ALL
High Amp Arc Ignition, HAI >= 120 arcs
@Thickness 1.50 mm
>= 120 arcs
@Thickness 0.0591 in
(ALL)
High Voltage Arc-Tracking Rate, HVTR 0.000 - 10.0 mm/min
@Thickness 3.00 mm
0.000 - 0.394 in/min
@Thickness 0.118 in
ALL
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 130 °C266 °F<20000 hours; IEC 60216-P1
 190 °C374 °F< 50 hours; IEC 60216-P1
Deflection Temperature at 8.0 MPa 70.0 °C158 °FISO 75-2
UL RTI, Electrical 105 °C
@Thickness 1.50 mm
221 °F
@Thickness 0.0591 in
(ALL)
UL RTI, Mechanical with Impact 130 °C
@Thickness 1.50 mm
266 °F
@Thickness 0.0591 in
(ALL)
UL RTI, Mechanical without Impact 130 °C
@Thickness 1.50 mm
266 °F
@Thickness 0.0591 in
(ALL)
Flammability, UL94 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
All colors
 
Processing PropertiesMetricEnglishComments
Feed Temperature 60.0 - 70.0 °C140 - 158 °FInjection molding
Nozzle Temperature 70.0 - 100 °C158 - 212 °FInjection molding
Melt Temperature 70.0 - 100 °C158 - 212 °FInjection molding
Mold Temperature 160 - 180 °C320 - 356 °FInjection molding
 160 - 180 °C320 - 356 °FCompression molding
Injection Pressure >= 10.0 MPa>= 1450 psiCompression and injection cavity mold pressure
Back Pressure 0.500 - 1.00 MPa72.5 - 145 psiInjection molding
Cure Time 0.167 - 0.333 min0.00278 - 0.00556 hourPer 1 mm of wall thickness, injection molding
 0.333 - 0.667 min0.00556 - 0.0111 hourPer 1 mm of wall thickness, compression molding
 
Descriptive Properties
Creep Rupture StrengthMedium
Holding PressureApproximately 40-60% of injection pressure
Media ResistanceMedium
Thermal ExpansionSlight
Water absorption (mg)7024h / 23°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Bakelite® UP 3415 Unsaturated Polyester Resin, Low Shrinkage, High Arc Resistance, UL Listed, High Mechanical Strength
Bakelite® UP 3420 Unsaturated Polyester Resin, High Mechanical Strength, High Arc Resistance, UL Listed, Low Shrinkage
Bakelite® UP 804 Unsaturated Polyester Resin, High Surface Quality, UL Listed, Low Shrinkage, High Arc Resistance
Bakelite® UP 3720 Unsaturated Polyester Resin, UL Listed, Low Shrinkage, High Arc Resistance
Bakelite® UP 802 Unsaturated Polyester Resin, High Surface Quality, Low Shrinkage, High Arc Resistance

PBAKE055 / 27089

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.