MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Sandvik 11R51 Spring Wire
Categories: Metal; Ferrous Metal; Special-Purpose Steel

Material Notes: Compared with standard grades Sandvik 12R10/gusab T302, Sandvik 11R51 offers:
  • higher tensile strength and tempering effect
  • higher relaxation resistance, especially at elevated temperatures
  • higher fatigue strength
  • better corrosion resistance, through the addition of molybdenum
  • Service temperature: -200 to 300°C (-330 to 570°F)

    Information provided by Sandvik

    ASTM 302; EN 1.4310

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Density 7.90 g/cc0.285 lb/in³
     
    Mechanical PropertiesMetricEnglishComments
    Tensile Strength, Ultimate  1505 MPa
    @Diameter 7.00 - 8.50 mm
    218300 psi
    @Diameter 0.276 - 0.335 in
     2530 MPa
    @Diameter 0.150 - 0.200 mm
    367000 psi
    @Diameter 0.00591 - 0.00787 in
    Tensile Strength, Yield  1280 MPa
    @Diameter 7.00 - 8.50 mm,
    Strain 0.2 %
    186000 psi
    @Diameter 0.276 - 0.335 in,
    Strain 0.2 %
     2150 MPa
    @Diameter 0.150 - 0.200 mm,
    Strain 0.2 %
    312000 psi
    @Diameter 0.00591 - 0.00787 in,
    Strain 0.2 %
    Modulus of Elasticity 185 GPa26800 ksias delivered
     190 GPa27600 ksias tempered
    Poissons Ratio 0.300.30Calculated
    Shear Modulus 71.0 GPa10300 ksias received
     73.0 GPa10600 ksias tempered
     
    Electrical PropertiesMetricEnglishComments
    Electrical Resistivity  0.0000900 ohm-cm
    @Temperature 20.0 °C
    0.0000900 ohm-cm
    @Temperature 68.0 °F
     0.0000950 ohm-cm
    @Temperature 100 °C
    0.0000950 ohm-cm
    @Temperature 212 °F
     0.000100 ohm-cm
    @Temperature 200 °C
    0.000100 ohm-cm
    @Temperature 392 °F
     0.000105 ohm-cm
    @Temperature 300 °C
    0.000105 ohm-cm
    @Temperature 572 °F
    Magnetic Permeability 3535µ
     
    Thermal PropertiesMetricEnglishComments
    CTE, linear  17.0 µm/m-°C
    @Temperature 20.0 - 100 °C
    9.44 µin/in-°F
    @Temperature 68.0 - 212 °F
     17.5 µm/m-°C
    @Temperature 20.0 - 200 °C
    9.72 µin/in-°F
    @Temperature 68.0 - 392 °F
     18.5 µm/m-°C
    @Temperature 20.0 - 300 °C
    10.3 µin/in-°F
    @Temperature 68.0 - 572 °F
    Specific Heat Capacity 0.500 J/g-°C
    @Temperature 50.0 - 100 °C
    0.120 BTU/lb-°F
    @Temperature 122 - 212 °F
    Thermal Conductivity  15.0 W/m-K
    @Temperature 20.0 °C
    104 BTU-in/hr-ft²-°F
    @Temperature 68.0 °F
     16.0 W/m-K
    @Temperature 100 °C
    111 BTU-in/hr-ft²-°F
    @Temperature 212 °F
     18.0 W/m-K
    @Temperature 200 °C
    125 BTU-in/hr-ft²-°F
    @Temperature 392 °F
     19.0 W/m-K
    @Temperature 300 °C
    132 BTU-in/hr-ft²-°F
    @Temperature 572 °F
    Maximum Service Temperature, Air 300 °C572 °F
    Minimum Service Temperature, Air -200 °C-328 °F
     
    Component Elements PropertiesMetricEnglishComments
    Carbon, C 0.080 %0.080 %
    Chromium, Cr 17 %17 %
    Iron, Fe 71.4 %71.4 %As Balance
    Manganese, Mn 1.8 %1.8 %
    Molybdenum, Mo 0.70 %0.70 %
    Nickel, Ni 7.5 %7.5 %
    Phosphorus, P <= 0.025 %<= 0.025 %
    Silicon, Si 1.5 %1.5 %
    Sulfur, S <= 0.015 %<= 0.015 %

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    AISI Type 304HN Stainless Steel
    Sandvik 12R10 Spring Wire
    Crucible Steel 416 Plus Chromium Steel
    ATI Allvac® VascoMax® T-250 Specialty Steel, Heat Treatment: 816°C (1500°F) + Age
    Eagle Brass 301 Austenitic Stainless Steel, Full Hardened

    NSANDV264 / 19158

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.