MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Celcon® CH15 Carbon Fiber Reinforced Acetal Copolymer
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Carbon Fiber Filled

Material Notes: Description: Celcon CH-15 is a special carbon fiber reinforced acetal copolymer for use in applications requiring electrical conductivity or static dissipation. It offers significantly higher strength and stiffness over Celcon EF10

Information provided by Celanese Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.44 g/cc0.0520 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 151 MPa21900 psi5 mm/min; ISO 527-2/1A
Elongation at Break 2.4 %2.4 %5 mm/min; ISO 527-2/1A
Flexural Modulus 11.78 GPa1709 ksiISO 178
Izod Impact, Notched (ISO) 6.50 kJ/m²3.09 ft-lb/in²ISO 180/1A
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 160 °C320 °FISO 75-1, -2
 
Processing PropertiesMetricEnglishComments
Melt Temperature 182 - 199 °C360 - 390 °F
Mold Temperature 77.0 - 93.0 °C171 - 199 °F
Drying Temperature 82.2 °C180 °F
Dry Time 3 hour3 hour
Injection Pressure 75.8 - 110 MPa11000 - 16000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Celcon® EC15C Conductive Grade Acetal Copolymer
Celanese Celcon® EF10 Acetal Copolymer, 10% Carbon Fiber
Celanese Celcon® TX90 Acetal Copolymer
Celanese Celcon® EC90PLUS Acetal Copolymer
Celanese Celcon® TX86 Ductile Acetal Copolymer

PHCW13 / 45954

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.