MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Toray TORAYCA™ 2701T-30V PBT/ABS, CF + GF
Categories: Polymer; Thermoplastic; ABS Polymer; ABS/Polyester Alloy; Polyester, TP; Polybutylene Terephthalate (PBT)

Material Notes: Short carbon fiber reinforced PBT, CF+GF, Flame retardant, PBT+ABS(CF+GF)20FR(17).

General Torayca™ Notes: TORAYCA™ is a carbon fiber reinforced thermoplastic (CFRTP) that is light weight and features excellent strength, stiffness, dimensional accuracy, and sliding properties. Physical property: Carbon fiber reinforced thermoplastic (CFRTP) offer excellent mechanical strength/rigidity and maintain a combination of characteristics. Lower specific gravity and lightweight, High creep resistance and fatigue resistance, Excellent abrasion resistance and sliding properties. Low molding shrinkage and coefficient of linear expansion, ensuring high dimensional accuracy, Excellent electrical conductivity and electromagnetic shielding performance.

Information provided by Toray Resin Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.217 g/cc0.04397 lb/in³ISO 1183
Filler Content 30 %30 %
Water Absorption 1.1 %1.1 %In 23°C water, polymer initially at 50% RH
Linear Mold Shrinkage, Flow 0.0010 cm/cm0.0010 in/in80x80x3mmt.; Toray Method
Linear Mold Shrinkage, Transverse 0.0050 cm/cm0.0050 in/in80x80x3mmt.; Toray Method
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 264 MPa
@Temperature 23.0 °C
38300 psi
@Temperature 73.4 °F
ISO 527-1,2
Elongation at Break 2.2 %
@Temperature 23.0 °C
2.2 %
@Temperature 73.4 °F
ISO 527-1,2
Flexural Strength 398 MPa
@Temperature 23.0 °C
57700 psi
@Temperature 73.4 °F
ISO 178
Flexural Modulus 20.0 GPa
@Temperature 23.0 °C
2900 ksi
@Temperature 73.4 °F
ISO 178
Charpy Impact, Notched 1.28 J/cm²
@Temperature 23.0 °C
6.09 ft-lb/in²
@Temperature 73.4 °F
V-Notched; ISO 179
Coefficient of Friction 0.360.36Vs S45C. 1 MPa, 0.33m/s; Suzuki Method
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1000 ohm-cm1000 ohm-cmIEC 60093
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 15.0 µm/m-°C8.33 µin/in-°FISO 11359-2
Melting Point 225 °C437 °FDSC Method
Deflection Temperature at 1.8 MPa (264 psi) 210 °C410 °FISO 75-1,2
Flammability, UL94 HBHB
 
Descriptive Properties
Amount of Wear (mg/h)0.3Vs S45C, 1 MPa, 0.33 m/s, Suzuki Method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTORAY9169 / 248858

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.