MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Colour Image Plastic Compound FRblend® PBT-1309 PBT, Carbon/Glass Fiber Reinforced, Flame Retardant
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Carbon Fiber Filled; Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant

Material Notes: Product Description: FRblend® PBT-1309 is a carbon and glass filled, flame retardant polybutylene -terephathalate compound. This grade offers good electrical properties and game resistance with balance mechanical properties.

Features:

  • Flame retardant
  • Good electrical properties
  • Balance mechanical properties
Uses:
  • Electrical/ electronic applications
Forms:
  • Pellets
Processing Method:
  • Injection Molding

Information provided by Colour Image Plastic Compound Sdn Bhd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.55 g/cc1.55 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0010 - 0.0020 cm/cm
@Thickness 3.20 mm
0.0010 - 0.0020 in/in
@Thickness 0.126 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 110 MPa16000 psiASTM D638
Elongation at Break 1.5 %1.5 %ASTM D638
Tensile Modulus 21.2 GPa3070 ksiASTM D638
Flexural Strength 180 MPa26100 psiASTM D790
Flexural Modulus 10.793 GPa1565.4 ksiASTM D790
Izod Impact, Notched 0.860 J/cm1.61 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 1000 - 1.00e+6 ohm1000 - 1.00e+6 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 202 °C
@Thickness 4.00 mm
396 °F
@Thickness 0.157 in
Unannealed; ASTM D648
Flammability, UL94 V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 230 - 240 °C446 - 464 °F
Middle Barrel Temperature 235 - 245 °C455 - 473 °F
Front Barrel Temperature 240 - 250 °C464 - 482 °F
Nozzle Temperature 250 - 260 °C482 - 500 °F
Mold Temperature 50.0 - 90.0 °C122 - 194 °F
Drying Temperature 80.0 - 100 °C176 - 212 °F
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCOLO064 / 265956

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.