MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Abadan Petrochemical MH (K-75) VAC Copolymer PVC Powder
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Powder

Material Notes: Used for flooring.

Information provided by Abadan Petrochemical Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.470 - 0.530 g/cc0.0170 - 0.0191 lb/in³
Volatiles 0.40 %0.40 %
Particle Mesh Size >= 42 Mesh>= 42 Mesh100% passes
 
Descriptive Properties
ColorWhite
Fish Eyes50/1000 cm3
Foreign Matter30 pcs/100 g PVC
Mean Polymerization Degree1400-1600
Residual Vinyl Chloride Monomer3 ppm by weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Geon® Performance Solutions 130 Series 136 Polyvinyl Chloride Copolymer (PVC Copolymer)
Geon® Performance Solutions 130 Series 138 Polyvinyl Chloride Copolymer (PVC Copolymer)
Geon® Performance Solutions 130 Series 137 Polyvinyl Chloride Copolymer (PVC Copolymer)
Formosa Plastics Formolon® 113 PVC
Inovyn 460SL Polyvinyl Chloride grafted copolymer

PIRABA989 / 197441

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.