System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Akro-Plastic Akrotek® PK-VM GF 40 8 black (6995) Polyketone, Glass Fiber
Categories:
Polymer
;
Thermoplastic
;
Polyketone
;
Polyketone, Glass Fiber Reinforced
Material Notes:
Compound for water contact. KTW, ACS, WRAS, NSF 61 hot water (GF 0 % –50 %). PK GF 40.
Information provided by Akro-Plastic GmbH
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.56
g/cc
0.0564
lb/in³
ISO 1183
Filler Content
40 %
40 %
ISO 1172
Linear Mold Shrinkage, Flow
0.0010
-
0.0030
cm/cm
0.0010
-
0.0030
in/in
ISO 294-4
Linear Mold Shrinkage, Transverse
0.0040
-
0.0060
cm/cm
0.0040
-
0.0060
in/in
ISO 294-4
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
140
MPa
20300
psi
Conditioned; ISO 527-2
150
MPa
21800
psi
Dry as Molded; ISO 527-2
Elongation at Break
2.3 %
2.3 %
Conditioned; ISO 527-2
2.3 %
2.3 %
Dry as Molded; ISO 527-2
Tensile Modulus
11.0
GPa
1600
ksi
1 mm/min. Conditioned; ISO 527-2
11.0
GPa
1600
ksi
1 mm/min. Dry as Molded.; ISO 527-2
Charpy Impact Unnotched
4.00
J/cm²
@Temperature 23.0 °C
19.0
ft-lb/in²
@Temperature 73.4 °F
Conditioned; ISO 179-1/1eA
5.00
J/cm²
@Temperature 23.0 °C
23.8
ft-lb/in²
@Temperature 73.4 °F
Dry as Molded; ISO 179-1/1eA
Charpy Impact, Notched
1.60
J/cm²
@Temperature 23.0 °C
7.61
ft-lb/in²
@Temperature 73.4 °F
Conditioned; ISO 179-1/1eA
1.60
J/cm²
@Temperature 23.0 °C
7.61
ft-lb/in²
@Temperature 73.4 °F
Dry as Molded; ISO 179-1/1eA
Thermal Properties
Metric
English
Comments
Melting Point
220
°C
428
°F
Dry as Molded. DES, 10°C/min; DIN EN 11357-1
Deflection Temperature at 1.8 MPa (264 psi)
220
°C
428
°F
Dry as Molded; ISO 75
Flammability, UL94
HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
Conditioned
HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
Dry as Molded
Descriptive Properties
Burning Rate
<100 mm/min
Dry as Molded. FMVSS 302. >1 mm thickness
<100 mm/min
Conditioned. FMVSS 302. >1 mm thickness
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PAKRO9918 / 255575
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.