MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

NOVA Chemicals SPs116-C Octene Copolymer sLLDPE Film Resin
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade; LLDPE/Octene, Film

Material Notes: Features: excellent seal properties, superior toughness with excellent tear strength, excellent optics. Common additives: processing antioxidant, polymer process aid, PPA.

Applications: Lamination film, co-extruded sealant layer, tie concentrate blend layer, liquid packaging.

Film properties reported are typical of blown film extruded on a 2.5" extruder with 4" die and 35-mil die gap at a blow up ratio of 2.5:1, but are dependent upon operating conditions.

Information provided by NOVA Chemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.916 g/cc0.0331 lb/in³ASTM D 792
Thickness 25.0 microns0.984 milAs tested
Melt Index of Compound 1.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
1.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D 1238
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 8.40 MPa1220 psiASTM D882
Film Tensile Strength at Yield, TD 8.60 MPa1250 psiASTM D882
Film Elongation at Break, MD 500 %500 %ASTM D882
Film Elongation at Break, TD 870 %870 %ASTM D882
Elmendorf Tear Strength MD 270 g
@Thickness 0.0250 mm
270 g
@Thickness 0.000984 in
ASTM D1922
Elmendorf Tear Strength TD 541 g
@Thickness 0.0250 mm
541 g
@Thickness 0.000984 in
ASTM D1922
Dart Drop Test 695 g
@Thickness 0.0250 mm
1.53 lb
@Thickness 0.000984 in
ASTM D1709/A
Film Tensile Strength at Break, MD 35.2 MPa5110 psiASTM D882
Film Tensile Strength at Break, TD 51.6 MPa7480 psiASTM D882
1% Secant Modulus, MD 160 MPa23200 psiASTM D882
1% Secant Modulus, TD 165 MPa23900 psiASTM D882
Heat Seal Strength Initiation Temperature 98.0 °C208 °FNOVA Chemicals test method
 
Optical PropertiesMetricEnglishComments
Haze 5.0 %
@Thickness 0.0250 mm
5.0 %
@Thickness 0.000984 in
ASTM D1003
Gloss 78 %
@Thickness 0.0250 mm
78 %
@Thickness 0.000984 in
ASTM D2457
 
Descriptive Properties
Low Friction Puncture105 J/mmNOVA Chemicals test

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOV610 / 249057

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.