MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Acrylic, Heat Resistant, Molded
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, Heat Resistant, Molded

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Heat Resistant, Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.15 - 1.20 g/cc0.0415 - 0.0434 lb/in³Average value: 1.18 g/cc Grade Count:21
Water Absorption 0.300 - 2.00 %0.300 - 2.00 %Average value: 0.436 % Grade Count:14
Water Absorption at Saturation 0.300 %0.300 %Average value: 0.300 % Grade Count:4
Linear Mold Shrinkage 0.00200 - 0.00700 cm/cm0.00200 - 0.00700 in/inAverage value: 0.00418 cm/cm Grade Count:19
Melt Flow 1.00 - 13.0 g/10 min1.00 - 13.0 g/10 minAverage value: 2.68 g/10 min Grade Count:21
Spiral Flow 27.0 - 30.0 cm10.6 - 11.8 inAverage value: 28.2 cm Grade Count:5
 130 - 220 cm
@Temperature 230 - 250 °C
51.2 - 86.6 in
@Temperature 446 - 482 °F
Average value: 175 cm Grade Count:1
 130 - 220 cm
@Thickness 2.00 - 2.00 mm
51.2 - 86.6 in
@Thickness 0.0787 - 0.0787 in
Average value: 175 cm Grade Count:1
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 44.0 - 10544.0 - 105Average value: 89.4 Grade Count:18
Tensile Strength, Ultimate 44.1 - 80.0 MPa6400 - 11600 psiAverage value: 69.7 MPa Grade Count:18
Tensile Strength, Yield 71.7 - 76.0 MPa10400 - 11000 psiAverage value: 74.4 MPa Grade Count:3
Elongation at Break 3.00 - 30.0 %3.00 - 30.0 %Average value: 10.4 % Grade Count:19
Elongation at Yield 4.00 - 13.0 %4.00 - 13.0 %Average value: 6.14 % Grade Count:7
Modulus of Elasticity 1.72 - 3.60 GPa250 - 522 ksiAverage value: 3.01 GPa Grade Count:19
Flexural Yield Strength 68.9 - 140 MPa10000 - 20300 psiAverage value: 109 MPa Grade Count:18
Flexural Modulus 1.79 - 3.60 GPa260 - 522 ksiAverage value: 3.01 GPa Grade Count:18
Izod Impact, Notched 0.157 - 0.534 J/cm0.294 - 1.00 ft-lb/inAverage value: 0.286 J/cm Grade Count:12
 0.240255 - 0.32034 J/cm
@Temperature 0.000 - 0.000 °C
0.450096 - 0.60013 ft-lb/in
@Temperature 32.0 - 32.0 °F
Average value: 0.274 J/cm Grade Count:4
Charpy Impact Unnotched 1.60 - 3.50 J/cm²7.61 - 16.7 ft-lb/in²Average value: 2.01 J/cm² Grade Count:8
Charpy Impact, Notched 0.120 - 0.300 J/cm²0.571 - 1.43 ft-lb/in²Average value: 0.150 J/cm² Grade Count:7
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 18.7 - 20.0 kV/mm475 - 508 kV/inAverage value: 19.6 kV/mm Grade Count:3
 
Thermal PropertiesMetricEnglishComments
CTE, linear 72.0 - 90.0 µm/m-°C
@Temperature 0.000 - 156 °C
40.0 - 50.0 µin/in-°F
@Temperature 32.0 - 312 °F
Average value: 76.5 µm/m-°C Grade Count:4
Thermal Conductivity 0.187 - 0.200 W/m-K1.30 - 1.39 BTU-in/hr-ft²-°FAverage value: 0.189 W/m-K Grade Count:7
Maximum Service Temperature, Air 98.0 - 118 °C208 - 244 °FAverage value: 108 °C Grade Count:6
Deflection Temperature at 0.46 MPa (66 psi) 94.4 - 113 °C202 - 235 °FAverage value: 102 °C Grade Count:8
Deflection Temperature at 1.8 MPa (264 psi) 85.0 - 108 °C185 - 226 °FAverage value: 97.4 °C Grade Count:14
Vicat Softening Point 95.0 - 240 °C203 - 464 °FAverage value: 114 °C Grade Count:21
Flammability, UL94 HBHBGrade Count:8
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.49 - 1.511.49 - 1.51Average value: 1.50 Grade Count:16
Haze 0.300 - 96.0 %0.300 - 96.0 %Average value: 8.24 % Grade Count:13
Yellow Index 0.300 - 5.50 %0.300 - 5.50 %Average value: 1.60 % Grade Count:4
Transmission, Visible 80.0 - 93.0 %80.0 - 93.0 %Average value: 90.8 % Grade Count:16
UV Transmittance 91.0 - 92.0 %91.0 - 92.0 %Average value: 91.8 % Grade Count:5
 
Processing PropertiesMetricEnglishComments
Melt Temperature 220 - 250 °C428 - 482 °FAverage value: 240 °C Grade Count:5
Mold Temperature 43.3 - 90.0 °C110 - 194 °FAverage value: 65.2 °C Grade Count:5
Drying Temperature 82.2 - 109 °C180 - 228 °FAverage value: 87.6 °C Grade Count:5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Acrylic, General Purpose, Molded
Overview of materials for Acrylic, Extruded
Trinseo Plexiglas® Diffuse™ V045-68207 Acrylic Resin
Trinseo Plexiglas® VS-UVT Acrylic
Trinseo Solarkote™ A200 Acrylic

O1304 / 77863

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.