MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Syensqo (Solvay Specialty Polymers) Torlon® AI-30 LM PAI, Low MDA version of AI-30
Categories: Polymer; Thermoplastic; Polyamide-imide (PAI)

Material Notes: Torlon® AI-30 LM is a wet polymer granule developed for the performance coatings industry. This polyamide-imide precursor consists of roughly 35% polymer solids, 63% water and 2% NMP. The high acid number of the polymer backbone allows the formulation of aqueous solutions with the addition of an appropriate complexing amine. Aqueous-based solutions made with Torlon® AI-30 LM have inherently low VOCs, which helps end users meet stringent environmental regulations.

Coatings based on the Torlon® AI-30 LM polymer yield durable, abrasion-resistant, thermally-stable films. The cured resin has superior resistance to organic solvents and a wide array of other commercial and industrial chemicals. Outstanding tribological characteristics are afforded both by the resin as well as its unparalleled intra-coat adhesion to fluoropolymers.

Aqueous-based AI-30 LM polymer coatings offer a sustainable solution for electrical/electronic, high temperature decorative and corrosion preventative applications. In addition, magnet wire insulation and protective coatings for printed circuit boards may be converted from solvent-borne (NMP) polyamide-imide solutions. Industrial applications include primers and decorative topcoats for cookware, appliances and housewares. Aqueous AI-30 LM polymer solutions may be easily combined with aqueous fluoropolymer dispersions to produce sustainable, high-performance, low-friction, corrosion-resistant coatings that provide protection to industrial and automotive parts.

Applications: Binder; Coating Applications

Features: Abrasion Resistant; Chemical Resistant; Flame Retardant; Good Adhesion; High Heat Resistance; Water Soluble

Solution Processing

Waterborne polyamide-imide solutions may be formulated using Torlon® AI-30 LM and an appropriate complexing amine. Please contact your Solvay representative for further details. Waterborne PAI solutions are patent protected (US 6,479,581).

Application

There are numerous methods by which waterborne Torlon® AI-30 LM resin-based coatings can be effectively applied. Depending on the aesthetic and performance characteristics required, uniform coatings can be applied by spray, roll, spin or curtain techniques. Usually, dry film thicknesses from 5-10 µm are readily achieved in a single coating pass, with multi-coat systems affording the opportunity for even further surface build. Regardless of the method employed, it is essential to assure appropriate preparation of the substrate prior to application of coating. Once complete, application equipment should be purged of the coating and cleaned with water.

Drying/Curing

Coatings based upon Torlon® AI-30 LM resin dry and initiate cure at temperatures as low as 150°C (300°F). However, optimal film properties result after heating for 5 to 20 minutes at 275°C (527°F), depending on the film thickness and the formulation. In the case of multi-coat systems, an intermediate temperature step at around 200°C (390°F) for 10 minutes may be advisable. For coating formulations employing low solids, a brief flash off period of about 3 to 10 minutes may be recommended prior to initiating cure.

Information provided by Solvay Specialty Polymers.

Vendors: Drake Plastics Ltd. Co. The Torlon Specialist, manufactures & stocks the most complete line of Torlon PAI in machinable rod, plate & Seamless Tube®. Drake works closely with Solvay Specialty Polymers to identify & serve a multitude of new applications. Drake, a lean producer of extruded, injection molded & machined shapes & parts, offers low minimums & quick, economical delivery globally.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Chemical PropertiesMetricEnglishComments
Total Acid Number 125125KOH/g
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorYellow
FormsPowder
ProcessingCoating; Solution Processing

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOL8Y4556 / 280356

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.