MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik Vestodur® X7085 45% Glass Fiber Reinforced PBT  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled

Material Notes: Description: VESTODUR X7085 is a 45 % glass fiber-reinforced, polymer-modified polybutylene terephthalate compound for injection molding. The compound is suitable for parts that are subjected to high mechanical and thermal loads. Compared with commonly used glass fiber-reinforced PBT compounds with similar stiffness parts of VESTODUR X7085 have in particular a high surface quality.

Information provided by degussa.

Evonik Industries is the successor company to Degussa.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.70 g/cc0.0614 lb/in³ISO 1183
Water Absorption at Saturation 0.40 %0.40 %ISO 62
Linear Mold Shrinkage 0.0015 cm/cm
@Thickness 2.00 mm
0.0015 in/in
@Thickness 0.0787 in
sheet with film gate at rim, mold temperature 80°C
Linear Mold Shrinkage, Transverse 0.013 cm/cm0.013 in/in
Melt Flow 20.4 g/10 min
@Load 2.16 kg,
Temperature 250 °C
20.4 g/10 min
@Load 4.76 lb,
Temperature 482 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 180 MPa26100 psiISO 527-1/2
Elongation at Break 1.8 %1.8 %ISO 527-1/2
Tensile Modulus 14.5 GPa2100 ksiISO 527-1/-2
Charpy Impact Unnotched  5.00 J/cm²
@Temperature -30.0 °C
23.8 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
 5.00 J/cm²
@Temperature 23.0 °C
23.8 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  1.30 J/cm²
@Temperature -30.0 °C
6.19 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 1.30 J/cm²
@Temperature 23.0 °C
6.19 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 223 °C433 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 210 °C410 °FISO 75-1/-2
Vicat Softening Point 210 °C410 °FMethod B, 50 N; ISO 306
 220 °C428 °FMethod A, 10 N; ISO 306
Flammability, UL94  HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in
IEC 60695
 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
IEC 60695

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Envalior Durethan® BCF 30 X H2.0 901510 Nylon 6 (PA6), 30% Glass/Carbon Fiber Reinforced, Dry
Mitsubishi Reny® 1012H Polyamide
Azoty Tarnow™ Tarnamid® T-27 GF50 Polyamide 6 - Glass Fiber Reinforced
Mitsubishi Reny® 2041 Polyamide
Evonik Vestodur® CL2045 45% Glass Reinforced, Crosslinkable PBT Based Compound

PHUMA62 / 47576

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.