MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Zoltek™ PX35 SW48-50 Woven Carbon Fiber Fabric
Categories: Carbon; Carbon Fiber/Carbon Fibre; Other Engineering Material; Composite Fibers

Material Notes: ZOLTEK PX35 Tow Weave Carbon Fabrics are produced from ZOLTEK PX35 50K Continuous Tow Carbon Fiber. Quick composite part build-up is cost effectively achieved with cosmetically attractive carbon fiber fabrics. Applications include large composite tooling parts and aesthetically appealing finished composite components.

Information provided by Zoltek Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.81 g/cc0.0654 lb/in³
Thickness 7.20 microns0.283 mil
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 4137 MPa600000 psiContinuous Tow
Elongation at Break 1.5 %1.5 %Continuous Tow
Tensile Modulus 242 GPa35100 ksiContinuous Tow
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00155 ohm-cm0.00155 ohm-cm
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 95 %95 %
 
Descriptive Properties
Areal Weight1640 g/m2
Construction5 harness satin weave
Fiber Diameter (µm)7.2
Fill Yarn2.4/cm
Roll Length25 m
Roll Width1.27 m
Warp Yarn2.6/cm
YarnZoltek PX35 50K tow with Epoxy sizing at 1.5%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Zoltek™ PX35 Multi-Directional Carbon Fiber Fabric
Zoltek™ PX35 UD150 Uni-Directional Carbon Fabric
Zoltek™ PX35 Continuous Tow Carbon Fiber
Zoltek™ PX35 P/TW28-50 Woven Carbon Fiber Fabric
Zoltek™ OX KF07 Knit Oxidized PAN Fiber Fabric

ECZO813 / 232281

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.