MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mitsubishi Chemical Advanced Materials Duratron™ T4203 PAI Extruded Polyamide-imide
Categories: Polymer; Thermoplastic; Polyamide-imide (PAI); Polyamide-Imide, Extruded

Material Notes: The ultimate PAI for impact strength and elongation, can bear high loads in extreme temperatures and offers exceptional dimensional stability and machinability.

Vendors: TriStar Plastics Corp. provides engineering, custom fabrication and manufacturing of high-performance plastics and self-lubricating bearing materials, such as Rulon, PEEK, Torlon, CJ Composites and Ultracomp. Capabilities include component design, material selection, prototype and production, manufacturing and surface modification. Call (800) TRI-STAR (800) 874-7827 or visit or www.TStar.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.41 g/cc1.41 g/ccASTM D792
Water Absorption at Saturation 1.70 %1.70 %ASTM D570 (17)
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell E 80.080.0ASTM D785
Hardness, Shore D 88.088.0ISO 868
Tensile Strength 150 MPa21800 psiISO 527-1/-2 (7)
Elongation at Yield 9.00 %9.00 %ISO 527-1/-2 (7)
Flexural Strength 178 MPa25800 psiISO 178 (12)
Compressive Yield Strength  34.0 MPa
@Strain 1.00 %
4930 psi
@Strain 1.00 %
ISO 604 (10)
 67.0 MPa
@Strain 2.00 %
9720 psi
@Strain 2.00 %
ISO 604 (10)
 135 MPa
@Strain 5.00 %
19600 psi
@Strain 5.00 %
ISO 604 (10)
Shear Strength 110 MPa16000 psiASTM D732
Charpy Impact, Notched 1.50 J/cm²7.14 ft-lb/in²ISO 179-1/1eA
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square 1.00e+14 ohm1.00e+14 ohmANSI/ESD STM 11.11
Dielectric Constant 4.20
@Frequency 1.00e+6 Hz
4.20
@Frequency 1.00e+6 Hz
ASTM D150
Dielectric Strength 22.8 kV/mm580 kV/inASTM D149
 24.0 kV/mm610 kV/inIEC 60243-1 (15)
Dissipation Factor 0.0260
@Frequency 1.00e+6 Hz
0.0260
@Frequency 1.00e+6 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear 37.8 µm/m-°C21.0 µin/in-°FASTM E-831 (TMA)
 40.0 µm/m-°C
@Temperature 23.0 - 100 °C
22.2 µin/in-°F
@Temperature 73.4 - 212 °F
 40.0 µm/m-°C
@Temperature 23.0 - 150 °C
22.2 µin/in-°F
@Temperature 73.4 - 302 °F
 50.0 µm/m-°C
@Temperature >=150 °C
27.8 µin/in-°F
@Temperature >=302 °F
Thermal Conductivity 0.259 W/m-K1.80 BTU-in/hr-ft²-°F
 0.260 W/m-K1.80 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 260 °C500 °FContinuous Use Temperature in Air after 20000 hr
Deflection Temperature at 1.8 MPa (264 psi) 278 °C532 °FASTM D648
Minimum Service Temperature, Air -50.0 °C-58.0 °F
Glass Transition Temp, Tg 275 °C527 °FDMA- Tan d
 
Chemical Resistance PropertiesMetricEnglishComments
Acids, Strong (pH 1-3) LimitedLimited
Acids, Weak AcceptableAcceptable
Alcohols AcceptableAcceptable
Alkalies, Strong (pH 11-14) UnacceptableUnacceptable
Alkalies, Weak LimitedLimited
Chlorinated Solvents AcceptableAcceptable
Continuous Sunlight LimitedLimited
Hot Water / Steam LimitedLimited
Hydrocarbons - Aliphatic AcceptableAcceptable
Hydrocarbons - Aromatic AcceptableAcceptable
Inorganic Salt Solutions AcceptableAcceptable
Ketones, Esters AcceptableAcceptable
 
Descriptive Properties
ESd categoryInsulative

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials Duratron™ T4301 PAI Polyamide-imide, extruded bearing grade
Mitsubishi Chemical Advanced Materials Duratron™ T4501 PAI Polyamide-imide, compression molded bearing grade
Mitsubishi Chemical Advanced Materials Duratron™ T5030 PAI Polyamide-imide, glass reinforced, extruded
Mitsubishi Chemical Advanced Materials Ketron™ 1000 PEEK, Extruded Unfilled Polyetherether Ketone
Mitsubishi Chemical Advanced Materials Duratron™ T4503 PAI Compression Molded, Polyamide-imide, Electrical Grade

P1SM38 / 20133

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.