MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Albis Plastics Polyamide 66 PA 910/1/ CF 10 GF10 HZ , 10% Carbon Fiber, 10% Glass Fiber, Impact Modified, DAM  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Glass/Carbon Fiber Filled

Material Notes: Semi-crystalline Nylon 66 (PA 66)

Characteristics: High Stiffness , Toughness and Electrically Conductive

Applications: Bearings, Gears, Conveyor Parts, Automotive Housings.

Processing: Injection Molding (Melt Temperature: 500-575°F, Mold Temperature: 175-250°F)

Data supplied by Albis Plastics Corporation.

Former ALBIS Plastics product lines have been spun off under the MOCOM brand. This specific grade was discontinued prior to the spin off.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.21 g/cc0.0437 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 133.8 MPa19410 psiASTM D638
Elongation at Break 2.7 %2.7 %ASTM D638
Modulus of Elasticity 9.52 GPa1380 ksiASTM D638
Flexural Modulus 8.00 GPa1160 ksiASTM D790
Izod Impact, Notched 1.17 J/cm2.19 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Melting Point 249 - 254 °C480 - 489 °FASTM D2117
Vicat Softening Point >= 200 °C>= 392 °F(VST/B/50); ASTM D1525
 
Processing PropertiesMetricEnglishComments
Melt Temperature 260 - 302 °C500 - 576 °FInjection
Mold Temperature 79.0 - 121 °C174 - 250 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient Edgetek® NN-10GF-10CF-20MN/000 Nylon 66 - 10% Glass Fiber/10% Carbon Fiber/20% Mineral - ESD Applications
Albis Plastics Polyamide 66 PA 910/1 CF 10 - 10% Carbon Fiber, DAM
Evonik Vestamid® DX9320 Black 10% Glass Reinforced Nylon 612 (Conditioned)
LG Chemical LUMID GP2101BF PA66+GF10%, Halogen Free Flame Retardant
Mocom (ALBIS) Vorprodukt® AL PA66 910/2.1 GF8 TCE8 Polyamide 66

PZA1B20 / 21708

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.