MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polymer Resources PC/ABS-GP1-[color]-3 PC Blend, General Purpose, UV-stabilized  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/Thermoplastic Polyurethane Blend; Polyurethane, TP

Material Notes: Process: Injection Molding
Notes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.

Information provided by Polymer Resources Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.15 g/cc0.0415 lb/in³ASTM D792
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm0.0050 - 0.0070 in/inASTM D955
Melt Flow 14 - 15 g/10 min14 - 15 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 53.8 MPa7800 psiASTM D638
Tensile Strength, Yield 52.4 MPa7600 psiASTM D638
Flexural Strength 72.4 MPa10500 psiASTM D790
Flexural Modulus 2.21 GPa320 ksiASTM D790
Izod Impact, Notched 4.81 J/cm9.00 ft-lb/inASTM D256
Gardner Impact >= 36.2 J>= 26.7 ft-lbASTM D3029
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 113 °C235 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 98.9 °C210 °FASTM D648
Flammability, UL94  HB
@Thickness 1.59 mm
HB
@Thickness 0.0625 in
 HB
@Thickness 3.17 mm
HB
@Thickness 0.125 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 249 - 288 °C480 - 550 °F
Middle Barrel Temperature 254 - 293 °C490 - 560 °F
Front Barrel Temperature 260 - 302 °C500 - 575 °F
Melt Temperature 274 - 302 °C525 - 575 °F
Mold Temperature 71.1 - 93.3 °C160 - 200 °F
Drying Temperature 76.7 - 82.2 °C170 - 180 °F
Dry Time 3 - 4 hour3 - 4 hour

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
PTS Tristar® PC-10GFR-(V) 10% Glass Reinforced UV Stabilized Polycarbonate With Release
Covestro Bayblend® T80 XG PC/ABS Blend
Multibase Multi-ABS 3075 High Impact
Covestro Bayblend® T65 AT PC/ABS Blend
Covestro Bayblend® KU 1-1446 Polycarbonate + ABS

PPOLYR053 / 57215

Polyurethane

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.