MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

Mitsubishi FGF Recycled PIPG Post-Industrial PET-G 3D Printing Polymer
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Renewable/Recycled Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); PETG Copolyester

Material Notes: FGF Recycled PIPG (Post-Industrial PET-G) is strong & flexible, odor neutral. This material shows very low shrinkage and almost no warping which makes it an excellent material, because it combines the advantages of both PLA and ABS.

Features:

  • Post Industrial Recycled Grade
  • Strong & Flexible
  • Limited Smell
  • Low “Warping “
Colors on request.

Information provided by Mitsubishi Chemical.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.25 g/cc1.25 g/ccISO 1183
Linear Mold Shrinkage 0.0037 cm/cm0.0037 in/inISO 294
Melt Flow 8.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
8.0 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ISO 1133
Storage Temperature 15.0 - 25.0 °C59.0 - 77.0 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 20.0 MPa2900 psiISO 527
Tensile Strength, Yield 49.0 MPa7110 psiISO 527
Elongation at Break 33 %33 %ISO 527
Elongation at Yield 4.0 %4.0 %ISO 527
Tensile Modulus 2.00 GPa290 ksiISO 527
Charpy Impact, Notched 0.260 J/cm²1.24 ft-lb/in²ISO 179
 
Processing PropertiesMetricEnglishComments
Zone 1 160 - 200 °C320 - 392 °F
Zone 2 180 - 220 °C356 - 428 °F
Zone 3 195 - 235 °C383 - 455 °F
Die Temperature 210 - 260 °C410 - 500 °F
Drying Temperature 65.0 °C149 °F<400 ppm
Dry Time 4.00 hour4.00 hour
 
Descriptive Properties
Mass Temperature219°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMITS9821 / 301046

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.