MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Epoxyset Epoxiohm EO-97M Electrically Conductive Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy, Electrically Conductive

Material Notes: EPOXIOHM-97M is one part, pure silver filled, high electrical conductivity, epoxy adhesive. It is designed for microelectronics chip bonding application.

Information provided by Epoxyset Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 3.20 g/cc0.116 lb/in³
Viscosity 10000 - 15000 cP10000 - 15000 cP
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8888ASTM D2240
Shear Strength 23.0 MPa3340 psi
Adhesive Bond Strength 8.96 MPa1300 psiLap Shear Strength
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity <= 0.000400 ohm-cm<= 0.000400 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 56.0 µm/m-°C31.1 µin/in-°F
Thermal Conductivity 2.00 W/m-K13.9 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 200 °C392 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F
Glass Transition Temp, Tg 89.0 °C192 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  10.0 min
@Temperature 175 °C
0.167 hour
@Temperature 347 °F
 120 min
@Temperature 125 °C
2.00 hour
@Temperature 257 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEPOXY818 / 150843

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.