MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Overview of materials for Thermoset Polyester, Mineral Filled
Categories: Polymer; Thermoset; Polyester, TS; Thermoset Polyester, Mineral Filled

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyester, Mineral Filled". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.59 - 2.08 g/cc0.0574 - 0.0751 lb/in³Average value: 1.89 g/cc Grade Count:13
Water Absorption 0.110 - 0.350 %0.110 - 0.350 %Average value: 0.215 % Grade Count:10
 0.400 - 0.400 %
@Temperature 50.0 - 50.0 °C
0.400 - 0.400 %
@Temperature 122 - 122 °F
Average value: 0.400 % Grade Count:1
 0.400 - 0.400 %
@Time 173000 - 173000 sec
0.400 - 0.400 %
@Time 48.0 - 48.0 hour
Average value: 0.400 % Grade Count:1
Linear Mold Shrinkage 0.00100 - 0.00910 cm/cm0.00100 - 0.00910 in/inAverage value: 0.00459 cm/cm Grade Count:13
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell E 61.0 - 78.061.0 - 78.0Average value: 69.0 Grade Count:10
Tensile Strength, Ultimate 24.1 - 79.3 MPa3500 - 11500 psiAverage value: 54.2 MPa Grade Count:13
Elongation at Break 0.410 - 1.11 %0.410 - 1.11 %Average value: 0.639 % Grade Count:10
Modulus of Elasticity 9.90 - 21.3 GPa1440 - 3090 ksiAverage value: 13.3 GPa Grade Count:10
Flexural Yield Strength 55.2 - 179 MPa8000 - 26000 psiAverage value: 101 MPa Grade Count:13
Flexural Modulus 8.96 - 19.9 GPa1300 - 2890 ksiAverage value: 12.2 GPa Grade Count:12
Compressive Yield Strength 117 - 194 MPa17000 - 28100 psiAverage value: 149 MPa Grade Count:13
Poissons Ratio 0.283 - 0.3300.283 - 0.330Average value: 0.302 Grade Count:6
Shear Modulus 3.87 - 7.71 GPa561 - 1120 ksiAverage value: 4.98 GPa Grade Count:6
Izod Impact, Notched 0.160 - 8.33 J/cm0.300 - 15.6 ft-lb/inAverage value: 1.39 J/cm Grade Count:13
Charpy Impact, Notched 0.180 - 0.276 J/cm²0.857 - 1.31 ft-lb/in²Average value: 0.238 J/cm² Grade Count:10
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 2.50e+14 - 6.60e+15 ohm-cm2.50e+14 - 6.60e+15 ohm-cmAverage value: 1.79e+15 ohm-cm Grade Count:10
Dielectric Constant 4.20 - 6.004.20 - 6.00Average value: 5.11 Grade Count:11
Dielectric Strength 10.2 - 15.7 kV/mm259 - 400 kV/inAverage value: 12.5 kV/mm Grade Count:13
Dielectric Breakdown 40.0 - 23000 V40.0 - 23000 VAverage value: 16900 V Grade Count:11
Dissipation Factor 0.0139 - 0.05000.0139 - 0.0500Average value: 0.0255 Grade Count:11
Arc Resistance 140 - 224 sec140 - 224 secAverage value: 188 sec Grade Count:13
Comparative Tracking Index 600 V600 VAverage value: 600 V Grade Count:10
 
Thermal PropertiesMetricEnglishComments
CTE, linear 46.0 - 76.0 µm/m-°C
@Temperature 40.0 - 130 °C
25.6 - 42.2 µin/in-°F
@Temperature 104 - 266 °F
Average value: 58.4 µm/m-°C Grade Count:9
Thermal Conductivity 0.700 - 0.760 W/m-K
@Temperature 100 - 100 °C
4.86 - 5.27 BTU-in/hr-ft²-°F
@Temperature 212 - 212 °F
Average value: 0.730 W/m-K Grade Count:3
Maximum Service Temperature, Air 167 - 218 °C333 - 424 °FAverage value: 192 °C Grade Count:10
Deflection Temperature at 1.8 MPa (264 psi) 174 - 260 °C345 - 500 °FAverage value: 218 °C Grade Count:12
Flammability, UL94 HB - V-0HB - V-0Grade Count:12
Oxygen Index 24.0 - 47.0 %24.0 - 47.0 %Average value: 30.1 % Grade Count:9

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for High Density Polyethylene (HDPE), Injection Molded
Overview of materials for Polyphenylene Sulfide (PPS) Alloy, Glass Reinforced, Flow Enhanced
Overview of materials for Thermoset Polyester Glass Filled BMC
RheTech Products P251-01 Polypropylene Copolymer, Black
Overview of materials for Polyester Thermoplastic Elastomer, Glass Filled

O3520 / 78221

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.