MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont™ Surlyn® 1601B-2 Sodium Ionomer Resin for Blown and Cast Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Ionomer; Ionomer, Film Grade

Material Notes: Surlyn® 1601 B-2 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Meat, poultry, seafood and cheese packaging; Cereal liners; Medical/pharmaceutical packaging; Powdered/granular food and nonfood pouches; Carded display/skin packaging films; Edible oil, motor oil, and other liquid product pouches; Snack structures

Data provided by the manufacturer, DuPont Packaging.

This product line/trade name was acquired by Dow, but this specific grade was discontinued prior to the acquisition.

Key Words: Ethylene/Methacrylic Acid (E/MAA) Copolymer
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.940 g/cc0.0340 lb/in³Estimated by MatWeb
Melt Flow 1.3 g/10 min
@Load 2.16 kg,
Temperature 190 °C
1.3 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 350 %350 %ASTM D882
Film Elongation at Break, TD 400 %400 %ASTM D882
Secant Modulus, MD 0.260 GPa37.7 ksiASTM D882
Secant Modulus, TD 0.0450 GPa6.53 ksiASTM D882
Impact 240240Spencer Impact in J/cm; ASTM D3420
Elmendorf Tear Strength, MD 0.900 g/micron22.9 g/mil
Elmendorf Tear Strength, TD 1.00 g/micron25.4 g/mil
Dart Drop 9.80 g/micron249 g/milASTM D1709B
Seal Strength 2600 g/25 mm2600 g/inSeal Bar Temp approx. 140-150°C
Hot Tack Strength 2100 g/25 mm2100 g/inSeal Bar Temp approx. 110-140°C; Packforsk Method
Film Tensile Strength at Break, MD 29.6 MPa4290 psiASTM D882
Film Tensile Strength at Break, TD 29.6 MPa4290 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point 98.0 °C208 °FDSC; ASTM D3418
Vicat Softening Point 74.0 °C165 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Haze 4.0 %4.0 %ASTM D1003
Gloss 65 %65 %20°; ASTM D2457
 
Processing PropertiesMetricEnglishComments
Melt Temperature 191 °C376 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow Surlyn® 1802 Sodium Ionomer Resin for Blown/Cast Film and Extrusion Coating
DuPont™ Surlyn® 1601B Sodium Ionomer Resin for Blown and Cast Film
Dow Surlyn® 1605 Sodium Ionomer Resin for Blown/Cast Film and Extrusion Coating
Dow Surlyn® 1601-2LM Sodium Ionomer Resin for Blown and Cast Film
Dow Surlyn® 1601 Sodium Ionomer Resin for Blown and Cast Film

PDU603 / 33080

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.