MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Gadolinium, Gd
Categories: Metal; Nonferrous Metal; Pure Element

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 7.89 g/cc0.285 lb/in³
 
Chemical PropertiesMetricEnglishComments
Atomic Mass 157.25157.251995
Atomic Number 6464
X-ray Absorption Edge 0.2468 Å0.2468 ÅK
 1.4787 Å1.4787 ÅLI
 1.56081 Å1.56081 ÅLII
 1.70955 Å1.70955 ÅLIII
Electronegativity 1.21.2Pauling
Ionic Radius 0.938 Å0.938 ÅCrystal Ionic Radius for Valence +3
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 3737polycrystalline
Tensile Strength, Ultimate 190 MPa27600 psi
Tensile Strength, Yield 173 MPa25100 psi
Elongation at Break 37 %37 %
Tensile Modulus 54.8 GPa7950 ksi
Bulk Modulus 37.9 GPa5500 ksi
Poissons Ratio 0.2590.259
Shear Modulus 21.8 GPa3160 ksiCalculated
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.000131 ohm-cm0.000131 ohm-cm
Magnetic Susceptibility 0.002260.00226cgs/g
Curie Temperature 20.0 °C68.0 °F
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 98.5 J/g42.4 BTU/lb
CTE, linear 9.40 µm/m-°C
@Temperature 100 °C
5.22 µin/in-°F
@Temperature 212 °F
Specific Heat Capacity 0.300 J/g-°C0.0717 BTU/lb-°F
Thermal Conductivity 8.80 W/m-K61.1 BTU-in/hr-ft²-°F
Melting Point 1310 - 1312 °C2390 - 2394 °F
Boiling Point 3273 °C5923 °F
 
Optical PropertiesMetricEnglishComments
Emissivity (0-1) 0.337
@Wavelength >=645 nm,
Temperature 1025 - 1313 °C
0.337
@Wavelength >=645 nm,
Temperature 1877 - 2395 °F
 
Component Elements PropertiesMetricEnglishComments
Gadolinium, Gd 100 %100 %
 
Descriptive Properties
CAS Number7440-54-2

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chromium, Cr; Recrystallized
Copper, Cu; Cold-Worked
Erbium, Er
Gold, Au
Americium, Am

AMEGd00 / 39

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.