MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Materion SupremEX® 217XG Aluminum - Silicon Carbide Metal Matrix Composite, T6 CWQ Forged Plate  (discontinued **)
Categories: Metal; Metal Matrix Composite; Nonferrous Metal; Aluminum Alloy; 2000 Series Aluminum Alloy

Material Notes: A high quality aerospace grade aluminum alloy (AA2124) reinforced with 17% sub-micron silicon carbide which is manufactured via a powder metallurgy route using a high energy mixing process to ensure a homogeneous distribution of the reinforcement and to refine the grain structure to enhance mechanical properties. The alloy is heat treatable offering high strength and modulus for structural applications and is available in billet, forged and extruded forms.

CWQ = Cold Water Quench

Information supplied by Materion.

Key Words: AlSiC. Designation: – 2124/SiC/17p
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.86 g/cc0.103 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 640 MPa92800 psi
Tensile Strength, Yield 540 MPa
@Strain 0.2 %
78300 psi
@Strain 0.2 %
Elongation at Break 4.0 %4.0 %
Modulus of Elasticity 98.0 GPa14200 ksi
Poissons Ratio 0.300.30
Shear Modulus 37.7 GPa5470 ksiCalculated
 
Thermal PropertiesMetricEnglishComments
CTE, linear 17.0 µm/m-°C9.44 µin/in-°F
Specific Heat Capacity 0.848 J/g-°C0.203 BTU/lb-°F
Thermal Conductivity 150 W/m-K1040 BTU-in/hr-ft²-°F
Melting Point >= 548 °C>= 1020 °F
Solidus 548 °C1020 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Materion SupremEX® 217XG Aluminum - Silicon Carbide Metal Matrix Composite, T6 HWQ Billet
Materion SupremEX® 217XG Aluminum - Silicon Carbide Metal Matrix Composite, T6 PGQ Billet
Materion SupremEX® 225XE Aluminum - Silicon Carbide Metal Matrix Composite, T6 PGQ Forged Plate
Materion SupremEX® 217XG Aluminum - Silicon Carbide Metal Matrix Composite, T6 CWQ Extruded Bar
Materion SupremEX® 225XE Aluminum - Silicon Carbide Metal Matrix Composite, T6 CWQ Billet

NBB9103 / 192324

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.