MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Glass Fiber Filled, Flame Retardant
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Glass Fiber Filled, Flame Retardant

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.13 - 1.48 g/cc0.0408 - 0.0535 lb/in³Average value: 1.32 g/cc Grade Count:22
Filler Content 10.0 - 30.0 %10.0 - 30.0 %Average value: 17.0 % Grade Count:5
Water Absorption 0.0700 - 0.300 %0.0700 - 0.300 %Average value: 0.223 % Grade Count:16
Linear Mold Shrinkage 0.00100 - 0.00600 cm/cm0.00100 - 0.00600 in/inAverage value: 0.00303 cm/cm Grade Count:18
Melt Flow 2.20 - 60.0 g/10 min2.20 - 60.0 g/10 minAverage value: 18.5 g/10 min Grade Count:6
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 103 - 116103 - 116Average value: 111 Grade Count:5
Tensile Strength, Ultimate 35.0 - 85.0 MPa5080 - 12300 psiAverage value: 61.6 MPa Grade Count:9
Tensile Strength, Yield 37.2 - 97.9 MPa5400 - 14200 psiAverage value: 65.5 MPa Grade Count:13
Elongation at Break 1.50 - 40.0 %1.50 - 40.0 %Average value: 7.29 % Grade Count:12
Modulus of Elasticity 3.10 - 9.65 GPa450 - 1400 ksiAverage value: 6.00 GPa Grade Count:5
Flexural Yield Strength 61.4 - 137 MPa8900 - 19900 psiAverage value: 98.4 MPa Grade Count:18
Flexural Modulus 2.00 - 7.86 GPa290 - 1140 ksiAverage value: 4.70 GPa Grade Count:22
Izod Impact, Notched 0.427 - 2.24 J/cm0.800 - 4.20 ft-lb/inAverage value: 0.742 J/cm Grade Count:15
Izod Impact, Unnotched 0.500 - 2.67 J/cm0.937 - 5.00 ft-lb/inAverage value: 1.96 J/cm Grade Count:8
Izod Impact, Notched (ISO) 5.00 - 15.0 kJ/m²2.38 - 7.14 ft-lb/in²Average value: 8.33 kJ/m² Grade Count:3
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+9 - 1.00e+16 ohm-cm1.00e+9 - 1.00e+16 ohm-cmAverage value: 2.18e+15 ohm-cm Grade Count:6
Dielectric Constant 3.30 - 3.703.30 - 3.70Average value: 3.47 Grade Count:4
Dielectric Strength 15.7 kV/mm400 kV/inAverage value: 15.7 kV/mm Grade Count:4
Dissipation Factor 0.01000.0100Average value: 0.0100 Grade Count:4
Comparative Tracking Index 300 - 600 V300 - 600 VAverage value: 500 V Grade Count:3
 
Thermal PropertiesMetricEnglishComments
CTE, linear 19.8 - 54.0 µm/m-°C11.0 - 30.0 µin/in-°FAverage value: 32.9 µm/m-°C Grade Count:7
Hot Ball Pressure Test 75.0 °C167 °FAverage value: 75.0 °C Grade Count:3
Deflection Temperature at 0.46 MPa (66 psi) 82.0 - 116 °C180 - 241 °FAverage value: 107 °C Grade Count:7
Deflection Temperature at 1.8 MPa (264 psi) 75.0 - 171 °C167 - 340 °FAverage value: 104 °C Grade Count:21
Vicat Softening Point 85.0 - 103 °C185 - 217 °FAverage value: 97.0 °C Grade Count:7
Flammability, UL94 V-0V-0Grade Count:18
Oxygen Index 27.0 - 37.0 %27.0 - 37.0 %Average value: 32.0 % Grade Count:4
Glow Wire Test 960 °C1760 °FAverage value: 960 °C Grade Count:4
 
Processing PropertiesMetricEnglishComments
Melt Temperature 180 - 240 °C356 - 464 °FAverage value: 213 °C Grade Count:8
Mold Temperature 40.0 - 93.3 °C104 - 200 °FAverage value: 66.7 °C Grade Count:10
Drying Temperature 80.0 - 85.0 °C176 - 185 °FAverage value: 81.3 °C Grade Count:9
Moisture Content 0.100 %0.100 %Average value: 0.100 % Grade Count:4
Dew Point -17.8 °C0.000 °FAverage value: -17.8 °C Grade Count:4
Injection Pressure 60.0 - 103 MPa8700 - 15000 psiAverage value: 84.3 MPa Grade Count:6

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded

O1110 / 77800

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.