MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil EXACT™ 4053 Plastomer for Film Applications
Categories: Polymer; Film; Thermoplastic; Elastomer, TPE; Thermoplastic Olefinic Elastomer (TPO), Film Grade; Polyethylene (PE)

Material Notes: Product Description: Exact 4053 is an ethylene-based butene plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. This resin is designed primarily for use in blends with polyolefines to improve the heat sealing performance and/or toughness in film applications. Exact 4053 contains no antioxidants.

Availability: Latin America, North America and South America

Additive:

  • Antiblock: No
  • Slip: No
  • Thermal Stabilizer: No
Applications:
  • Blend Partner
  • Blown Film

Data provided by the manufacturer, Exxon Chemical.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.888 g/cc0.0321 lb/in³Exxon Method
Thickness 25.4 microns1.00 mil
Melt Flow 2.2 g/10 min2.2 g/10 minExxon Method
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 3.52 MPa511 psiASTM D882
Film Tensile Strength at Yield, TD 3.10 MPa450 psiASTM D882
Film Elongation at Break, MD 530 %530 %ASTM D882
Film Elongation at Break, TD 760 %760 %ASTM D882
Film Elongation at Yield, MD 10 %10 %ASTM D882
Film Elongation at Yield, TD 10 %10 %ASTM D882
Secant Modulus, MD 0.0669 GPa9.70 ksiASTM D882
Secant Modulus, TD 0.0758 GPa11.0 ksiASTM D882
Elmendorf Tear Strength, MD 1.97 g/micron50.0 g/milASTM D1922
Elmendorf Tear Strength, TD 5.12 g/micron130 g/milASTM D1922
Dart Drop 5.51 g/micron140 g/milASTM D-1709
Film Tensile Strength at Break, MD 57.2 MPa8300 psiASTM D882
Film Tensile Strength at Break, TD 49.6 MPa7190 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point 70.0 °C158 °FPeak Melting, Exxon Method
 
Optical PropertiesMetricEnglishComments
Haze 1.6 %1.6 %ASTM D1003
Gloss 85 %85 %45; ASTM D-2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil Santoprene® 521-70 Thermoplastic Rubber
ExxonMobil Vyram™ 9201-75 Thermoplastic Elastomer
ExxonMobil EXACT™ SLP-9053 Plastomer for Compounding and Polymer Modification
ExxonMobil EXACT™ 8210 Plastomer for Multilayer Film Applications
ExxonMobil EXACT™ 8201 Plastomer for Blown Film Applications

PEXCIE / 38034

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.