MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Raschig Group MELOPLAS® 150 MF
Categories: Polymer; Thermoset; Melamine; Melamine-Phenolic Copolymer; Phenolic

Material Notes: Wood flour-reinforced MF molding compound in dark colors. High surface hardness, high mechanical strength, good electrical properties. Self-extinguishing (V-O/1,6 according to UL 94), UL-listed. Free of halogens and toxic heavy metals. Supervised according ISO 14528-3 DIN 7708: MF 150 ISO 800: MF B20 ISO 14528-3: MF (WD30+MD15) - (WD40+MD05). Forms: Low dust granulate packed in moisture resistant bags Standard bag size: 25 kg palletized in 1.000 kg loads or big-bags. Processing: Injection or compression. Applications: Molded parts in electrical engineering. Fittings for household appliances. Car ash-trays.

Information provided by the Raschig Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.50 - 1.70 g/cc1.50 - 1.70 g/ccISO 1183
Apparent Bulk Density 0.500 - 0.700 g/cc0.0181 - 0.0253 lb/in³ISO 60
Water Absorption <= 2.0 %
@Temperature 23.0 °C,
Time 86400 sec
<= 2.0 %
@Temperature 73.4 °F,
Time 24.0 hour
ISO 62
Linear Mold Shrinkage 0.0050 - 0.010 cm/cm0.0050 - 0.010 in/in(longitudinal) Compression; ISO 2577
 0.0080 - 0.013 cm/cm0.0080 - 0.013 in/in(longitudinal) Injection; ISO 2257
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 40.0 - 50.0 MPa5800 - 7250 psiCompression; ISO 527
 50.0 - 75.0 MPa7250 - 10900 psiInjection; ISO 527
Modulus of Elasticity 5.00 - 8.00 GPa725 - 1160 ksiInjection and Compression; ISO 527
Flexural Strength 70.0 - 100 MPa10200 - 14500 psiCompression; ISO 178
 90.0 - 120 MPa13100 - 17400 psiInjection; ISO 178
Flexural Modulus 8.00 - 9.00 GPa1160 - 1310 ksiInjection and Compression; ISO 178
Compressive Strength 200 - 250 MPa29000 - 36300 psiInjection and Compression; ISO 604
Charpy Impact Unnotched  0.500 - 0.700 J/cm²
@Temperature 23.0 °C
2.38 - 3.33 ft-lb/in²
@Temperature 73.4 °F
Compression; ISO 179/ 1eU
 0.700 - 1.00 J/cm²
@Temperature 23.0 °C
3.33 - 4.76 ft-lb/in²
@Temperature 73.4 °F
Injection; ISO 179/ 1eU
Charpy Impact, Notched  0.120 - 0.180 J/cm²
@Temperature 23.0 °C
0.571 - 0.857 ft-lb/in²
@Temperature 73.4 °F
Compression; ISO 179/ 1eA
 0.130 - 0.200 J/cm²
@Temperature 23.0 °C
0.619 - 0.952 ft-lb/in²
@Temperature 73.4 °F
Injection; ISO 179/ 1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+11 - 1.00e+12 ohm-cm1.00e+11 - 1.00e+12 ohm-cmIEC 60093
Surface Resistance 1.00e+10 - 1.00e+11 ohm1.00e+10 - 1.00e+11 ohmIEC 60093
Dielectric Constant  7.0 - 9.0
@Frequency 1e+6 Hz
7.0 - 9.0
@Frequency 1e+6 Hz
IEC 60250
 11 - 16
@Frequency 100 Hz
11 - 16
@Frequency 100 Hz
IEC 60250
Dielectric Strength 15.0 - 20.0 kV/mm381 - 508 kV/inIEC 60243-1
Dissipation Factor  0.030 - 0.050
@Frequency 1e+6 Hz
0.030 - 0.050
@Frequency 1e+6 Hz
IEC 60250
 0.30 - 0.50
@Frequency 100 Hz
0.30 - 0.50
@Frequency 100 Hz
IEC 60250
Arc Resistance 115 - 125 sec115 - 125 secASTM D495
Comparative Tracking Index >= 600 V>= 600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 15.0 - 35.0 µm/m-°C
@Temperature 50.0 - 100 °C
8.33 - 19.4 µin/in-°F
@Temperature 122 - 212 °F
longitudinal; ISO 11359-2
Thermal Conductivity 0.400 - 0.500 W/m-K2.78 - 3.47 BTU-in/hr-ft²-°FASTM E1461
Maximum Service Temperature, Air 135 °C275 °F20,000 h; IEC 60216/T1
 160 °C320 °F< 50 h; IEC 60216/T1
Deflection Temperature at 1.8 MPa (264 psi) 155 - 180 °C311 - 356 °FInjection and Compression; ISO 75
Deflection Temperature at 8.0 MPa 110 - 130 °C230 - 266 °FInjection and Compression; ISO 75
Flammability, UL94  V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
 5VB
@Thickness 1.50 mm
5VB
@Thickness 0.0591 in
Shrinkage 1.0 - 1.5 %
@Temperature 110 °C,
Time 605000 sec
1.0 - 1.5 %
@Temperature 230 °F,
Time 168 hour
ISO 2577
 
Processing PropertiesMetricEnglishComments
Shelf Life 6.00 Month
@Temperature 15.0 - 25.0 °C
6.00 Month
@Temperature 59.0 - 77.0 °F
 
Descriptive Properties
Arc resistance5 StufeASTM D495
Glow wire flammability test960/1IEC 60695 2-12
Glow wire ignitability test900/1IEC 60695 2-13
Water Absorption<115 mgISO 62; 24h / 23°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Plenco 3509 Phenolic, Granular, Transfer Molded
Dow HPL 502 Carboxylated Terpolymer Latex
Plenco 00714 Melamine-Phenolic, Granular, Injection Molded
Devcon Backing Compound Epoxy
CHT Group EP RP EPI Engineered Polymers Aromatic Polyurea

PRASCH23 / 65308

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.