MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Arla MULTICLEAR® BOX 2 WALL PC Sheet
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Optical Grade

Material Notes: MULTICLEAR® BOX 2 WALL is an aesthetically pleasing twin wall extruded multiwall polycarbonate sheet which offers higher light transmission products with lower weight for handling and transportation. MULTICLEAR® BOX 2 WALL is transparent and translucent with one side UV protected sheet (also available with two side UV protection, except 4-6 mm). Standard colors are clear, opal and bronze. Available in thicknesses of 4, 6, 8 and 10 mm. Knife cutting operation is used both online and offline to avoid saw dust. MULTICLEAR® BOX 2 WALL has a 10 year limited warranty against discoloration, loss of impact strength and light transmission due to weathering.

Benefits: High light transmission; Excellent bending radius; One side UV protection as standard; Light weight - simple handling and installation

Application: Building industry – roofing, cladding, sidewalls, conservatories, domes, skylights, sheds, car ports, smoke vents, swimming pool covers, suspended ceilings, glasshouses, shopping center roofing, railway/metro station, stadia roofing and partitions. Lighting/packaging lamp optics and neon signs boxes, pallet shields, protective covers for fragile items. Advertising illuminated signs and advertising panels. Agriculture greenhouses, lorry/tractor ports and farm/barn buildings.

Information provided by Arla Plast.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³ISO 1183
Moisture Absorption 0.150 %
@Time 86400 sec
0.150 %
@Time 24.0 hour
50% RH; ISO 62
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 7070ISO 2039-2
Tensile Strength at Break 70.0 MPa10200 psiISO 527
Tensile Strength, Yield 63.0 MPa9140 psiISO 527
Elongation at Break 110 %110 %ISO 527
Elongation at Yield 6.0 %6.0 %ISO 527
Modulus of Elasticity 2.30 GPa334 ksiISO 527
Flexural Modulus 2.30 GPa334 ksiISO 178
Izod Impact, Notched (ISO)  10.0 kJ/m²
@Temperature -30.0 °C
4.76 ft-lb/in²
@Temperature -22.0 °F
ISO 180/1A
 65.0 kJ/m²
@Temperature 23.0 °C
30.9 ft-lb/in²
@Temperature 73.4 °F
ISO 180/1A
Charpy Impact Unnotched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/2D
 NB
@Temperature -40.0 °C
NB
@Temperature -40.0 °F
ISO 179/2D
 
Thermal PropertiesMetricEnglishComments
CTE, linear 70.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
38.9 µin/in-°F
@Temperature 73.4 - 176 °F
Specific Heat Capacity 0.00117 J/g-°C0.000280 BTU/lb-°F
Thermal Conductivity 0.210 W/m-K1.46 BTU-in/hr-ft²-°FDIN 52612
Deflection Temperature at 0.46 MPa (66 psi) 142 °C288 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 132 °C270 °FISO 75
Vicat Softening Point 148 °C298 °FB 50; ISO 306
 149 °C300 °FB 120; ISO 306
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.5861.586ISO 489

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PARLA919 / 301097

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.