MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Zoltek™ PX35 Multi-Directional Carbon Fiber Fabric
Categories: Carbon; Carbon Fiber/Carbon Fibre; Other Engineering Material; Composite Fibers

Material Notes: ZOLTEK PX35 Multi-Axial Fabric is produced from ZOLTEK PX35 continuous carbon fiber tow. Unique fiber spreading techniques are utilized to obtain a wide range of MD fabric weights for a varied set of composite part applications. Quick composite part build-up is cost effectively achieved with a diverse weight range of low-cost carbon fiber products. Drapable fabric construction, ideal for complex shape performs. Pillar and Tricot stitching patterns available.

APPLICATIONS: • Automotive • Marine • Aircraft • Infrastructure.

RECOMMENDED USE: • Body Panels (Interior/Exterior) • Components/Undercarriage • Reinforcement.

Information provided by Zoltek Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.81 g/cc0.0654 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 4137 MPa600000 psi
Tensile Modulus 242 GPa35100 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00155 ohm-cm0.00155 ohm-cm
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 95 %95 %
 
Descriptive Properties
Fiber Diameter (µm)7.2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Zoltek™ PX35 SW48-50 Woven Carbon Fiber Fabric
Zoltek™ PX35 Type-02 Chopped Carbon Fiber
Zoltek™ PX35 Type-55 Chopped Carbon Fiber
Zoltek™ PX35 Continuous Tow Carbon Fiber
Solvay CYCOM® 934 Epoxy - Pitch High Modulus Carbon Fiber Reinforced Unidirectional Tape Laminate

ECZO820 / 232289

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.