MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mocom (ALBIS) ALTECH® ABS A 3230/516 GK20 GF10 ABS, 30% Glass Fibers/Glass Beads Reinforced
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled; Acrylonitrile Butadiene Styrene (ABS), Glass Bead Filled

Material Notes: Base Polymer: Acrylonitrile Butadiene Styrene Copolymer

Filler/Additive System: 30% Glass Fibers/Glass Beads

Color: Black

Special Features: Impact modified, high stiffness, processing stabilized

Application Area: Various

Typical Application: Various

Information provided by Albis Plastics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.26 g/cc0.0455 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cm
@Time 86400 sec
0.0020 - 0.0040 in/in
@Time 24.0 hour
ISO 294-4
Linear Mold Shrinkage, Transverse 0.0030 - 0.0050 cm/cm
@Time 86400 sec
0.0030 - 0.0050 in/in
@Time 24.0 hour
ISO 294-4
Melt Flow 11 g/10 min
@Load 10.0 kg,
Temperature 220 °C
11 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 97.0 MPa14100 psiH358/30; ISO 2039-1
Tensile Strength at Break 39.0 MPa5660 psiISO 527
Elongation at Break 1.7 %1.7 %ISO 527
Tensile Modulus 3.30 GPa479 ksiISO 527
Flexural Strength 62.0 MPa8990 psiISO 178
Flexural Modulus 4.00 GPa580 ksiISO 178
Charpy Impact Unnotched 1.30 J/cm²6.19 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 0.450 J/cm²2.14 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C185 °FISO 75-1/-2
Vicat Softening Point 93.0 °C199 °FB50; ISO 306
 
Processing PropertiesMetricEnglishComments
Melt Temperature 220 - 260 °C428 - 500 °FInjection molding
Mold Temperature 50.0 - 80.0 °C122 - 176 °FInjection molding
Drying Temperature  80.0 °C
@Time 7200 - 14400 sec
176 °F
@Time 2.00 - 4.00 hour
in a dry air (desiccant) dryer
 80.0 °C
@Time 10800 - 21600 sec
176 °F
@Time 3.00 - 6.00 hour
in an circulating dryer
 
Descriptive Properties
Base PolymerAcrylonitrile Butadiene Styrene Copolymer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PALBIS8624 / 242683

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.