MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Silicon, Si
Categories: Metal; Nonferrous Metal; Other Engineering Material; Semiconductor; Pure Element

Material Notes: Physical Form: Gray Crystals or Brown Amorphous Solid

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density  2.3016 g/cc
@Temperature 1027 °C
0.083151 lb/in³
@Temperature 1881 °F
 2.3077 g/cc
@Temperature 827 °C
0.083371 lb/in³
@Temperature 1520 °F
 2.3136 g/cc
@Temperature 627 °C
0.083584 lb/in³
@Temperature 1160 °F
 2.3192 g/cc
@Temperature 427 °C
0.083786 lb/in³
@Temperature 801 °F
 2.3269 g/cc
@Temperature 127 °C
0.084065 lb/in³
@Temperature 261 °F
 2.329 g/cc
@Temperature 25.0 °C
0.08414 lb/in³
@Temperature 77.0 °F
 2.533 g/cc
@Temperature 1412 °C
0.09151 lb/in³
@Temperature 2574 °F
Liquid (10% expansion upon freezing)
Viscosity 0.88 cP
@Temperature 1412 °C
0.88 cP
@Temperature 2574 °F
Liquid
a Lattice Constant 5.43072 Å5.43072 Å
Volume Compressibility, 10^-10 m²/N 0.3060.306
Surface Tension 736 dynes/cm
@Temperature 1412 °C
736 dynes/cm
@Temperature 2574 °F
Liquid
 
Chemical PropertiesMetricEnglishComments
Atomic Mass 28.085528.08551995
Atomic Number 1414
Thermal Neutron Cross Section 0.13 barns/atom0.13 barns/atom
X-ray Absorption Edge 6.7446 Å6.7446 ÅK
 105.05 Å105.05 ÅLI
 126.48 Å126.48 ÅLII
 126.48 Å126.48 ÅLIII
Critical Pressure 537 bar403000 torr
Critical Density 0.1207 g/cc0.004361 lb/in³
Critical Molar Volume 232.6 cm³/mol14.19 in³/mol
Electrode Potential -0.450 V-0.450 V
Electronegativity 1.91.9Pauling
Ionic Radius 0.420 Å0.420 ÅCrystal Ionic Radius for Valence +4
 0.650 Å0.650 ÅCrystal Ionic Radius for Valence +1
 2.71 Å2.71 ÅCrystal Ionic Radius for Valence -4
 3.84 Å3.84 ÅCrystal Ionic Radius for Valence -1
 
Mechanical PropertiesMetricEnglishComments
Knoop Microhardness 1127011270N/mm² Microhardness
Hardness, Mohs 7.07.0
Modulus of Elasticity 112.4 GPa16300 ksi
Compressive Strength 120 MPa17400 psi
Bulk Modulus 98.74 GPa14320 ksi
Poissons Ratio 0.280.28
Shear Modulus 43.9 GPa6370 ksiCalculated
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0100 ohm-cm0.0100 ohm-cm
Magnetic Susceptibility -0.00000390-0.00000390Atomic (cgs)
Critical Superconducting Temperature 6.70 - 7.10 K
@Pressure 12000 - 13000 MPa
6.70 - 7.10 K
@Pressure 1.74e+6 - 1.89e+6 psi
Dielectric Constant 11.811.8
Band Gap 1.107 eV1.107 eV
Electron Mobility, cm²/V-s 19001900
Hole Mobility, cm²/V-s 500500
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 1800 J/g774 BTU/lb
Heat of Vaporization 10610 J/g4566 BTU/lb
CTE, linear  2.49 µm/m-°C
@Temperature 25.0 °C
1.38 µin/in-°F
@Temperature 77.0 °F
 3.61 µm/m-°C
@Temperature 227 °C
2.01 µin/in-°F
@Temperature 441 °F
 4.15 µm/m-°C
@Temperature 527 °C
2.31 µin/in-°F
@Temperature 981 °F
 4.44 µm/m-°C
@Temperature 1027 °C
2.47 µin/in-°F
@Temperature 1881 °F
Specific Heat Capacity 0.794 J/g-°C0.190 BTU/lb-°FGas
 0.115 J/g-°C
@Temperature -213 °C
0.0275 BTU/lb-°F
@Temperature -351 °F
 0.259 J/g-°C
@Temperature -173 °C
0.0619 BTU/lb-°F
@Temperature -279 °F
 0.557 J/g-°C
@Temperature -73.0 °C
0.133 BTU/lb-°F
@Temperature -99.4 °F
 0.713 J/g-°C
@Temperature 27.0 °C
0.170 BTU/lb-°F
@Temperature 80.6 °F
 0.785 J/g-°C
@Temperature 127 °C
0.188 BTU/lb-°F
@Temperature 261 °F
 0.832 J/g-°C
@Temperature 227 °C
0.199 BTU/lb-°F
@Temperature 441 °F
 0.849 J/g-°C
@Temperature 327 °C
0.203 BTU/lb-°F
@Temperature 621 °F
 0.866 J/g-°C
@Temperature 427 °C
0.207 BTU/lb-°F
@Temperature 801 °F
 0.883 J/g-°C
@Temperature 527 °C
0.211 BTU/lb-°F
@Temperature 981 °F
 0.899 J/g-°C
@Temperature 627 °C
0.215 BTU/lb-°F
@Temperature 1160 °F
 0.916 J/g-°C
@Temperature 727 °C
0.219 BTU/lb-°F
@Temperature 1340 °F
 0.933 J/g-°C
@Temperature 827 °C
0.223 BTU/lb-°F
@Temperature 1520 °F
 0.950 J/g-°C
@Temperature 927 °C
0.227 BTU/lb-°F
@Temperature 1700 °F
 0.967 J/g-°C
@Temperature 1027 °C
0.231 BTU/lb-°F
@Temperature 1881 °F
 0.983 J/g-°C
@Temperature 1127 °C
0.235 BTU/lb-°F
@Temperature 2061 °F
 1.00 J/g-°C
@Temperature 1227 °C
0.239 BTU/lb-°F
@Temperature 2241 °F
 1.01 J/g-°C
@Temperature 1412 °C
0.241 BTU/lb-°F
@Temperature 2574 °F
Liquid
Thermal Conductivity 124 W/m-K861 BTU-in/hr-ft²-°F
 20.9 W/m-K
@Temperature 1200 °C
145 BTU-in/hr-ft²-°F
@Temperature 2190 °F
 37.7 W/m-K
@Temperature 600 °C
261 BTU-in/hr-ft²-°F
@Temperature 1110 °F
 52.3 W/m-K
@Temperature 400 °C
362 BTU-in/hr-ft²-°F
@Temperature 752 °F
 66.94 W/m-K
@Temperature 1412 °C
463.8 BTU-in/hr-ft²-°F
@Temperature 2574 °F
Liquid
 79.5 W/m-K
@Temperature 200 °C
551 BTU-in/hr-ft²-°F
@Temperature 392 °F
 105 W/m-K
@Temperature 100 °C
725 BTU-in/hr-ft²-°F
@Temperature 212 °F
Melting Point 1412 °C2574 °F
Boiling Point 3265 °C5909 °F
Heat of Formation 0.000 kJ/mol0.000 kJ/molCrystal
 450 kJ/mol450 kJ/molGas
Debye Temperature 372 °C702 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 3.493.49
Reflection Coefficient, Visible (0-1) 0.30 - 0.700.30 - 0.70varies irregularly with wavelength.
 
Component Elements PropertiesMetricEnglishComments
Silicon, Si 100 %100 %
 
Descriptive Properties
CAS Number7440-21-3
Crystal StructureCubicDiamond Structure - Space Group Fd3m
SolubilityInsoluble in H2O and Acid; Soluble in Alkaline

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Titanium, Ti
Copper, Cu; Annealed
Copper, Cu; Cold Drawn
Aluminum, Al
Nickel, Ni

AMESi00 / 102

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.