MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Plaskolite West Optix® CA-81 UVA-7 UV-Absorbing Acrylic Resin
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, UV Stabilized, Molded

Material Notes: Special UV-absorption grade, extrusion and injection molding

Applications: A special UV-absorption acrylic resin for extrusion and injection molding. It is slightly lubricated for ease of processing. This resin offers high heat resistance and excellent stiffness/strength properties with its polymer molecular weight being one of the highest among the CA acrylic resins.

Yellowness Index <7.0 per ASTM D1925.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.18 - 1.20 g/cc0.0426 - 0.0434 lb/in³ASTM D792
Melt Flow 2.0 - 3.0 g/10 min2.0 - 3.0 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 65.5 MPa9500 psiASTM D638
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 90.0 - 100 °C194 - 212 °FASTM D648
Vicat Softening Point 103 - 114 °C217 - 237 °FRate A, ASTM D1525
 
Optical PropertiesMetricEnglishComments
Haze 3.0 %3.0 %ASTM D1003
Transmission, Visible 91 %91 %ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Plaskolite West Optix® CA-81 UVA UV-Absorbing Acrylic Resin
Plaskolite West Optix® CA-1000 I Clear High Impact Acrylic Resin
Plaskolite West Optix® CA-86 Clear General Purpose Acrylic Resin
Plaskolite West Optix® CA-927 G HF Clear Impact Modified Acrylic Resin
Plaskolite West Optix® CA-927 HF Clear Impact Modified Acrylic Resin

PCA140 / 27902

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.