MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Arkema VOLTALEF® 300 HD PCTFE  (discontinued **)
Categories: Polymer; Thermoplastic; Fluoropolymer; Polychlorotrifluoroethylene (PCTFE); Molded

Material Notes: VOLTALEF® 300 HD is a chlorotrifluoroethylene powder. Used for compression molding, very good flow, non-flammable.

Information provided by Arkema Group

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 2.11 - 2.16 g/cc0.0762 - 0.0780 lb/in³ASTM D1050-68
Apparent Bulk Density 0.400 - 0.500 g/cc0.0145 - 0.0181 lb/in³
Particle Size 500 - 600 µm500 - 600 µm
Deformation 1.0 %1.0 %7 MPa load for 24 hrs at 25°C; ASTM D621
 2.5 %2.5 %7 MPa load for 24 hrs at 70°C; ASTM D621
 12 %12 %7 MPa load for 24 hrs at 125°C; ASTM D621
 
Mechanical PropertiesMetricEnglishComments
Hardness, H358/30 80.0 MPa11600 psiDIN 53456
Hardness, Shore D 75 - 9075 - 90ASTM D676
Tensile Strength, Ultimate 32.0 - 40.0 MPa4640 - 5800 psiASTM D638
 13.0 - 16.0 MPa
@Temperature 120 °C
1890 - 2320 psi
@Temperature 248 °F
ASTM D638
Tensile Strength, Yield 34.0 - 50.0 MPa4930 - 7250 psiASTM D638
 3.00 - 6.00 MPa
@Temperature 120 °C
435 - 870 psi
@Temperature 248 °F
ASTM D638
Elongation at Break 100 - 250 %100 - 250 %ASTM D638
Tensile Modulus 1.40 GPa203 ksiASTM D638
Flexural Modulus 1.40 GPa203 ksiASTM D790-80
Compressive Yield Strength 11.0 - 14.0 MPa1600 - 2030 psi1% deformation; ISO 604
 40.0 - 45.0 MPa5800 - 6530 psi0.2% off set; ISO 604
Compressive Modulus 1.40 GPa203 ksiASTM D638
Izod Impact, Notched 0.800 J/cm1.50 ft-lb/inASTM D256-81
Coefficient of Friction 0.26 - 0.450.26 - 0.45on polished steel
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.20e+18 ohm-cm1.20e+18 ohm-cmASTM D257-78
Dielectric Constant 2.4 - 3.0
@Frequency 100 - 1.00e+8 Hz
2.4 - 3.0
@Frequency 100 - 1.00e+8 Hz
ASTM D150
Dielectric Strength  15.0 kV/mm
@Thickness 3.20 mm
381 kV/in
@Thickness 0.126 in
stepwise tension increase; ASTM D149-75
 21.0 kV/mm
@Thickness 1.60 mm
533 kV/in
@Thickness 0.0630 in
continuous tension; ASTM D149-75
 48.0 kV/mm
@Thickness 0.760 mm
1220 kV/in
@Thickness 0.0299 in
stepwise tension increase; ASTM D149-75
 200 kV/mm
@Thickness 0.130 mm
5080 kV/in
@Thickness 0.00512 in
stepwise tension increase; ASTM D149-75
Arc Resistance 360 sec360 secASTM D495-73
 
Thermal PropertiesMetricEnglishComments
CTE, linear  55.0 µm/m-°C
@Temperature -80.0 - 70.0 °C
30.6 µin/in-°F
@Temperature -112 - 158 °F
ASTM D686-79
 250 µm/m-°C
@Temperature 70.0 - 150 °C
139 µin/in-°F
@Temperature 158 - 302 °F
ASTM D686-79
Specific Heat Capacity 0.900 J/g-°C0.215 BTU/lb-°F
Thermal Conductivity 0.135 W/m-K0.937 BTU-in/hr-ft²-°FF 433
Maximum Service Temperature, Air 150 °C302 °Fcontinuous service
 200 °C392 °Fpeak
Oxygen Index 100 %100 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Trinseo Plexiglas® VS-UVT Acrylic
Overview of materials for Polychlorotrifluoroethylene; Molded
Isoflon PCTFE Polychlorotrifluoroethylene
Daikin NEOFLON® M-300H PCTFE Granular Molding Powder
Arkema VOLTALEF® 302 PCTFE

PARKG684 / 24530

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.