MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Ateva® 1062 Ethylene Vinyl Acetate Copolymer Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade

Material Notes: Laminating and coextrusion; excellent sealability, opticals, strength, and antiblocking characteristics.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.926 g/cc0.0335 lb/in³ASTM D1505
Vinyl Acetate Content 6.0 %6.0 %
Melt Flow 1.8 g/10 min1.8 g/10 minASTM D1238 Cond. E
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 9.00 MPa1310 psiASTM D882
Film Tensile Strength at Yield, TD 9.00 MPa1310 psiASTM D882
Film Elongation at Break, MD 360 %360 %ASTM D882
Film Elongation at Break, TD 500 %500 %ASTM D882
Secant Modulus, MD 0.120 GPa17.4 ksiASTM D882
Secant Modulus, TD 0.125 GPa18.1 ksiASTM D882
Coefficient of Friction 0.750.75ASTM D1894
Dart Drop Test 90.0 g0.198 lbThickness not specified @ 50% Fail, ASTM D1709
Film Tensile Strength at Break, MD 23.0 MPa3340 psiASTM D882
Film Tensile Strength at Break, TD 16.0 MPa2320 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point 104 °C219 °FASTM D3417
 
Optical PropertiesMetricEnglishComments
Haze 7.0 %7.0 %ASTM D2457
Gloss 64 %64 %45° Gloss, ASTM D2457
 
Processing PropertiesMetricEnglishComments
Processing Temperature 160 - 210 °C320 - 410 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Ateva® 1941C Ethylene Vinyl Acetate Copolymer Packaging Resin
Arkema Evatane® 1005 VG 2 Ethylene Vinyl Acetate
Arkema Evatane® 1003 VL 2 Ethylene Vinyl Acetate
Arkema Evatane® 1020 VG 5 Ethylene Vinyl Acetate
Arkema Orevac® 9304 Film EVA-MAH Terpolymer

PATEVA05 / 25922

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.