MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BEC Materials SBS 791H
Categories: Polymer; Thermoplastic; Styrene-Butadiene; Styrene/Butadiene/Styrene (SBS)

Material Notes: Description: SBS rubber 791H is a special grade for asphalt modification with linear molecular structure and the styrene content of 30%. Its molecular weight is higher than that of grade 791 while fluidity is a little weaker. SBS polymer 791H is polystyrene(S)-polybutadiene(B)-polystyrene(S) triblock copolymer.

Application: Adhesives/Asphalt modification/Compounding

Formula: Asphalt Modification (Parts by mass)
SBS(YH791H): 4
Asphalt: 100
Antioxygen: 0.8

Information provided by BEC Materials, LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles <= 1.0 %<= 1.0 %
Melt Flow 0.010 - 0.50 g/10 min0.010 - 0.50 g/10 min
Ash <= 0.20 %<= 0.20 %
 
Chemical PropertiesMetricEnglishComments
Styrene Content 30 %30 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A >= 68>= 68
Tensile Strength >= 18.0 MPa>= 2610 psi
Elongation at Break >= 700 %>= 700 %
300% Modulus >= 2.00 MPa>= 290 psi
 
Descriptive Properties
Oil Content0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBECM053 / 307006

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.