MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF ecovio® FT2331 PLA
Categories: Polymer; Thermoplastic; Polylactic Acid (PLA) Biopolymer

Material Notes: Product Description: ecovio® FT2331 is our new biodegradable film product based on renewable resources. It is basically a compound of our biodegradable copolyester grades ecoflex® F and polylactic acid (PLA). Due to its outstanding mechanical strength ecovio® F2331 offers a great down gauging potential needed for very thing film applications like vegetable bags, organic waste bags etc. ecovio® F2331 already contains antiblocking and slip agents required for improved processing on film extrusion and film conversion equipment. Due to the high ecoflex® content in the continuous phase of the polymer structure, ecovio® F2331 exhibits very good sealing properties required for mono- and multi-layer films.

Availability: Europe; North America

Additive: Antiblock; Slip

Features: Antiblocking; Biodegradable; Compostable; Food Contact Acceptable; High Strength; Renewable Resource Content; Slip

Use: Bags; Blown Film; Packaging

Agency Ratings: ASTM D6400; DIN EN 13432; EC 1907/2006 (REACH); ; EC 2002/72/EC; FDA FCN 178; FDA FCN 475; FDA FCN 907

RoSH Compliance: RoSH Compliant

Form: Pellets

Processing Method: Blown Film

Information provided by BASF Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.780 g/cc0.0282 lb/in³ISO 60
Density 1.24 - 1.26 g/cc0.0448 - 0.0455 lb/in³ISO 1183
Melt Flow 8.0 - 12 g/10 min
@Load 5.00 kg,
Temperature 190 °C
8.0 - 12 g/10 min
@Load 11.0 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength  37.0 MPa
@Thickness 0.0305 mm
5370 psi
@Thickness 0.00120 in
MD, Blown Film; ISO 527-3
 40.0 MPa
@Thickness 0.0305 mm
5800 psi
@Thickness 0.00120 in
TD, Blown Film; ISO 527-3
Film Elongation at Break, MD 550 %
@Thickness 0.0305 mm
550 %
@Thickness 0.00120 in
Blown Film; ISO 527-3
Film Elongation at Break, TD 600 %
@Thickness 0.0305 mm
600 %
@Thickness 0.00120 in
Blown Film; ISO 527-3
Tensile Modulus  0.130 GPa
@Thickness 0.0305 mm
18.9 ksi
@Thickness 0.00120 in
TD, Blown Film; ISO 527-3
 0.200 GPa
@Thickness 0.0305 mm
29.0 ksi
@Thickness 0.00120 in
MD, Blown Film; ISO 527-3
Dart Drop Test 500 g
@Thickness 0.0305 mm
1.10 lb
@Thickness 0.00120 in
Blown Film; ASTM D1709A
 
Thermal PropertiesMetricEnglishComments
Melting Point 110 - 120 °C230 - 248 °Fecoflex®
 140 - 155 °C284 - 311 °FPLA

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBASG2156 / 310849

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.