MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Zoltek™ PX35 Milled Carbon Fiber
Categories: Carbon; Carbon Fiber/Carbon Fibre; Other Engineering Material; Composite Fibers

Material Notes: ZOLTEK’s PX35 Milled Fibers are specifically processed PAN (polyacrylonitrile) based fibers for lower cost applications. All ZOLTEK milled products are free of any sizings. ZOLTEK’s in-house milling system ensures product quality and traceability from raw material through finished product.

APPLICATIONS: • RFI/EMI shielding of electronic devices • Buoyancy • Static dissipation • Resin-rich surface reinforcement in composites • Low-cost friction compounds.

Information provided by Zoltek Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.490 g/cc0.0177 lb/in³
Density 1.81 g/cc0.0654 lb/in³
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00155 ohm-cm0.00155 ohm-cm
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 95 %95 %
 
Descriptive Properties
Fiber Diameter (µm)7.2
Fiber Length100 µm(MF150. Average)
 150 µm (MF200. Average)
Filament ShapeRound
Linear Resistivity (Omega;/cm)0.0761

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Zoltek™ PX35 UD150 Uni-Directional Carbon Fabric
E-Glass Fiber, Generic
Carlisle 201LL Carbon-Carbon Composite
Sinotek Materials Packing Carbon Fiber with Graphite
A-Glass Fiber, Generic

ECZO814 / 232282

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.