MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultramid® 1C PA6/66 (Dry)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6/66; Nylon 66/6, Unreinforced

Material Notes: Description: Ultramid® 1C forms flexible, scratch-resistant coatings or tough, resilient, abrasion-resistant coverings on plastics, films, nonwovens, fabrics, leather, paper, wood, or metal.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.500 - 0.800 g/cc0.0181 - 0.0289 lb/in³
Density 1.10 g/cc0.0397 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 115 MPa16700 psiISO 2039/1
Tensile Modulus 2.40 GPa348 ksiISO 527
Flexural Strength 100 MPa14500 psiISO 178
Flexural Modulus 2.30 GPa334 ksiISO 178
Charpy Impact Unnotched 15.0 J/cm²71.4 ft-lb/in²ISO 179/1eU
 
Thermal PropertiesMetricEnglishComments
Melting Point 185 °C365 °F
Glass Transition Temp, Tg 73.0 °C163 °F
Decomposition Temperature >= 300 °C>= 572 °F
Ignition Temperature >= 400 °C>= 752 °FASTM D1929
 
Descriptive Properties
Commercial StatusEurope

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® 1C PA6/66 (Conditioned)
Celanese Zytel® ST801 NC010A PA66-HI
Domo Technyl® B 50H1 Nylon 66/6, Flame Retardant, EH50
Kolon KOPA® KN1322VO Flame Retardant Nylon 6
Celanese Zytel® 101L NC010 PA66

PBASG0356 / 131989

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.