MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Plenco 1510 Polyester, Pellet, Injection Molded  (discontinued **)
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Polyester, TS; Thermoset Polyester, Mineral Filled

Material Notes: PLENCO 01510 is a mineral filled, pelletized polyester molding compound, which offers an excellent combination of electrical properties and dimensional stability. UL recognized under component file E40654. 01510 is available in black.

Information supplied by Plenco.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.960 g/cc0.0347 lb/in³ASTM D1895
Density 2.02 g/cc0.0730 lb/in³ASTM D792
Water Absorption 0.126 %0.126 %ASTM D570
Linear Mold Shrinkage 0.0038 cm/cm0.0038 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell E 7272ASTM D785
Tensile Strength, Ultimate 74.0 MPa10700 psiASTM D638
Elongation at Break 0.51 %0.51 %ASTM D638
Tensile Modulus 21.3 GPa3090 ksiASTM D638
Flexural Strength 114 MPa16500 psiASTM D790
Flexural Modulus 19.1 GPa2770 ksiASTM D790
Compressive Strength 155 MPa22500 psiASTM D695
Izod Impact, Notched 0.220 J/cm0.412 ft-lb/inASTM D256
Charpy Impact, Notched 0.227 J/cm²1.08 ft-lb/in²ASTM D256
Impact 126126J/m Drop Ball Impact; PLENCO
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 3.70e+15 ohm-cm3.70e+15 ohm-cmASTM D247
Dielectric Constant 4.64.6ASTM D150
Dielectric Strength 11.5 kV/mm292 kV/inStep by Step; ASTM D149
 15.3 kV/mm389 kV/inShort Time; ASTM D149
Dielectric Breakdown 23000 V23000 V1hr 120C; ASTM D149
Dissipation Factor 0.01530.0153ASTM D150
Arc Resistance 191 sec191 secASTM D495
Comparative Tracking Index 600 V600 VASTM D3638
 
Thermal PropertiesMetricEnglishComments
CTE, linear 48.0 µm/m-°C
@Temperature 40.0 - 130 °C
26.7 µin/in-°F
@Temperature 104 - 266 °F
TMA; ASTM E831
Maximum Service Temperature, Air 215 °C419 °FHeat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 249 °C480 °FASTM D648
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
Oxygen Index 24.5 %24.5 %ASTM D2863
Shrinkage 0.00182 %0.00182 %72 hr, 120ºC; ASTM D1299

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Plenco 1501 Polyester, Briquette, Transfer Molded
Celanese Celstran® PP-GF60-25 AD3002 Black PP, 60% Glass Reinforced
Plenco 1500 Polyester, Granular, Transfer Molded
Plenco 1500 Polyester, Granular, Compression Molded
LATI Larpeek 10 GCE/600 PEEK, Glass/Mineral Reinforced

PLEL20 / 50588

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.