MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Guang Dong LH-PS680 Conductive PS
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Extrusion Grade

Material Notes: Application Field: Suitable for injecting carrier tape disc, turnover box, electronic packaging products, electrical and electronic components.

Feature: Low water absorption rate, good thermal stability, good toughness, high impact and good liquidity, dimensional stability

Grade: Injection Grade

Information provided by GuangDong LuHua New Material Technology Holding Co

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.10 - 1.14 g/cc1.10 - 1.14 g/ccGB/T1033
Melt Flow 0.30 g/10 min
@Load 5.00 kg,
Temperature 210 °C
0.30 g/10 min
@Load 11.0 lb,
Temperature 410 °F
GB/T3682
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 17.62 MPa2556 psiGB/T1040-1992
Flexural Strength 23.36 MPa3388 psiGB/T9341-2008
Flexural Modulus 0.97598 GPa141.55 ksiGB/T9341-2008
Tensile Impact Strength 2.093 kJ/m²0.9959 ft-lb/in²GB/T1843-80
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 1000 ohm - 1e+051000 ohm - 1e+05GB/T1410

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGDON020 / 283968

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.