MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SCG Chemicals PG770 PVC Paste Resin
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Powder

Material Notes: SCG™ PVC PG770 is a high molecular weight homopolymer paste PVC resin, produced by TPC Paste Resin Co., Ltd. under OxyChem’s HYBRID technology.

Applications: High strength top skin layer for synthetic leather, high strength tarpaulins, strand coating products, mesh coating products, fabric coating products, metal coating products, disposable glove, industrial glove, auto sealants, logo, flow molding products, toys or rotational molding products, boots or slush molding products, terminal sleeve, printing ink, crown closure, other high physical strength PVC products.

Features: Low viscosity and good viscosity stability. Good air release properties. Excellent heat stability. Very high physical strength.

Information provided by SCG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles 0.30 %
@Temperature 110 °C
0.30 %
@Temperature 230 °F
ISO-1269
Viscosity 10200 cP
@Temperature 25.0 °C
10200 cP
@Temperature 77.0 °F
Severs Viscosity 2 hours after mixing, DOP 60 phr; RY-W-QC-E030
Brookfield Viscosity 2700 cP
@Temperature 23.0 °C
2700 cP
@Temperature 73.4 °F
20 rpm, 2 hours after mixing, DOP 60phr; ASTM D1824
 
Descriptive Properties
AppearanceWhite powder
Degree of Polymerization1870refer JIS K 6721
K Value79ISO 1628-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSCGC837 / 278094

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.