MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Toyobo CoolPoly® D5120 PPS
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS); Molded

Material Notes: Product Description: CoolPoly D series of thermally conductive plastics transfers heat, a characteristic previously unavailable in injection molding grade polymers. CoolPoly is lightweight, netshape moldable and allows design freedom in applications previously restricted to metals. The D series is electrically non-conductive and can be used for its dielectric properties.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.00 g/cc0.0723 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.0020 cm/cm0.0020 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.0050 cm/cm0.0050 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 100100ISO 2039-2
Tensile Strength at Break 125 MPa18100 psiISO 527-2/5
Elongation at Break 0.80 %0.80 %ISO 527-2/5
Tensile Modulus 16.0 GPa2320 ksiISO 527-1
Flexural Strength 190 MPa27600 psiISO 178
Flexural Modulus 18.0 GPa2610 ksiISO 178
Charpy Impact Unnotched 1.30 J/cm²6.20 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 0.357 J/cm²1.70 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.706 W/m-K4.90 BTU-in/hr-ft²-°FFlow; ASTM D1461
 0.706 W/m-K4.90 BTU-in/hr-ft²-°FThruplane; ASTM D1461
Deflection Temperature at 0.46 MPa (66 psi) 280 °C536 °FUnannealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 260 °C500 °FUnannealed; ISO 75-2/A
Flammability, UL94 V-0
@Thickness 1.52 mm
V-0
@Thickness 0.0600 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 295 - 315 °C563 - 599 °F
Middle Barrel Temperature 270 - 325 °C518 - 617 °F
Front Barrel Temperature 305 - 345 °C581 - 653 °F
Nozzle Temperature 300 - 330 °C572 - 626 °F
Zone 4 305 - 345 °C581 - 653 °FInjection
Melt Temperature 300 - 330 °C572 - 626 °F
Mold Temperature 135 - 175 °C275 - 347 °F
Drying Temperature 150 °C302 °F
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hour
Back Pressure <= 0.703 MPa<= 102 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHCQ6269 / 310962

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.