MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik VESTAMID® LC-GF30 NC Nylon 12, 30% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12); Nylon 12, 30% Glass Fiber Filled

Material Notes: VESTAMID® LC-GF30 NC is a semi-crystalline, heat- and UV-stabilized compound based on PA 12 from which connectors are preferrably produced by injection molding. The polyamide compound is especially suitable for the automotive and mobility sector. The semi-crystalline molding compound absorbs only small amounts of water. Components made from VESTAMID® LC-GF30 NC therefore have excellent dimensional accuracy with changing ambient humidity and constant general chemical stability. The semi-crystalline polymer is characterized by its outstanding mechanical and thermal load capacity. Molding or process-specific deviations from the recommended processing parameters are possible to a certain extent if the cavity or the process requires it. VESTAMID® LC-GF30 NC is delivered as cylindrical-granules in ready-to-process condition, in moisture-tight packaging. Preliminary data sheet.
Dry properties listed below
Industrial Sector: Automotive and Mobility, Industry and Engineering
Processing: Injection molding
Delivery form: Pellets, Granules
Optics: Laser absorbing
Resistance to: Heat (thermal stability), UV / light / weathering
Electrical: Insulating
Conformity: Automotive
Additives: Glass fibers
Applications: Quick-connectors
Special Characteristics: Halogen-free, Semi-crystalline, U.V. stabilized, Medium viscosity
Features: Lightweight, Non-corrosive
Color: Natural color
Additives: Light stabilizer
Delivery form: Cylindrical pellets
Chemical Resistance: Fuel resistance

Information provided by Evonik.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.24 g/cc0.0448 lb/in³ISO 1183
Viscosity Number 172 cm³/g1.72 dl/gCorrected; ISO 307, 1157, 1628
Linear Mold Shrinkage, Flow 0.00200 cm/cm0.00200 in/inISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.00800 cm/cm0.00800 in/inISO 294-4, 2577
Melt Flow 23.0 g/10 min
@Load 5.00 kg,
Temperature 275 °C
23.0 g/10 min
@Load 11.0 lb,
Temperature 527 °F
ISO 1133
Spiral Flow 40.2 cm15.8 inCross Section 6 x 2 mm2
 50.7 cm20.0 in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 80.080.0ISO 7619-1
Tensile Strength at Break 116 MPa16800 psiISO 527
Tensile Strength, Yield 120 MPa17400 psiISO 527
Elongation at Break 6.00 %6.00 %Nominal; ISO 527
 7.00 %7.00 %ISO 527
Elongation at Yield 5.00 %5.00 %ISO 527
Tensile Modulus 6.92 GPa1000 ksiISO 527
Charpy Impact Unnotched  9.80 J/cm²
@Temperature 23.0 °C
46.6 ft-lb/in²
@Temperature 73.4 °F
Type of failure: C; ISO 179/1eU
 10.2 J/cm²
@Temperature -30.0 °C
48.5 ft-lb/in²
@Temperature -22.0 °F
Type of failure: C; ISO 179/1eU
 10.6 J/cm²
@Temperature -40.0 °C
50.4 ft-lb/in²
@Temperature -40.0 °F
Type of failure: C; ISO 179/1eU
Charpy Impact, Notched  1.80 J/cm²
@Temperature -40.0 °C
8.57 ft-lb/in²
@Temperature -40.0 °F
Type of failure: C; ISO 179/1eA
 1.90 J/cm²
@Temperature -30.0 °C
9.04 ft-lb/in²
@Temperature -22.0 °F
Type of failure: C; ISO 179/1eA
 2.70 J/cm²
@Temperature 23.0 °C
12.8 ft-lb/in²
@Temperature 73.4 °F
Type of failure: C; ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 178 °C352 °FISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 179 °C354 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 165 °C329 °FISO 75-1/-2
Vicat Softening Point  174 °C
@Load 5.10 kg
345 °F
@Load 11.2 lb
50 K/h; ISO 306
 177 °C
@Load 1.02 kg
351 °F
@Load 2.25 lb
50 K/h; ISO 306
Glass Transition Temp, Tg 43.0 °C109 °FISO 11357-1/-2
 
Processing PropertiesMetricEnglishComments
Feed Temperature 40.0 - 60.0 °C104 - 140 °F
Nozzle Temperature 260 °C500 °FInjection Molding
Zone 1 260 °C500 °FInjection Molding
Zone 2 260 °C500 °FInjection Molding
Zone 3 260 °C500 °FInjection Molding
Zone 4 50.0 °C122 °FInjection Molding
Melt Temperature 250 °C482 °Fflow spiral
 240 - 280 °C464 - 536 °FInjection Molding
 260 °C500 °F
Mold Temperature 80.0 °C176 °Fflow spiral
 60.0 - 100 °C140 - 212 °FInjection Molding
 80.0 °C176 °F
Injection Velocity 950 mm/sec37.4 in/secflow front, flow spiral
Drying Temperature 80.0 - 100 °C176 - 212 °FPre-drying
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourPre-drying
Moisture Content 0.0540 %0.0540 %ISO 15512
Injection Pressure 150 MPa21800 psiflow spiral
 200 MPa29000 psiflow spiral
Back Pressure 0.300 - 0.800 MPa43.5 - 116 psiInjection Molding
Screw Speed 127 rpm127 rpmInjection Molding
 
Descriptive Properties
ColorNatural Color

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEVONIK7914 / 325046

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.