MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

A-Glass Fiber, Generic
Categories: Ceramic; Glass; Glass Fiber; Oxide; Silicon Oxide; Other Engineering Material; Composite Fibers

Material Notes: Used as a reinforcing agent in fiber glass composites, including biomedical/surgical applications.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.44 g/cc0.0882 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 3310 MPa480000 psi
Elongation at Break 4.8 %4.8 %
Modulus of Elasticity 68.9 GPa9990 ksi
Poissons Ratio 0.1830.183
Shear Modulus 29.1 GPa4220 ksiCalculated
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+8 ohm-cm1.00e+8 ohm-cm
Dielectric Constant 6.2
@Frequency 1e+6 Hz
6.2
@Frequency 1e+6 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 9.00 µm/m-°C
@Temperature 20.0 °C
5.00 µin/in-°F
@Temperature 68.0 °F
Specific Heat Capacity 0.796 J/g-°C0.190 BTU/lb-°F
Softening Point 727 °C1340 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.5381.538

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
E-Glass Fiber, Generic
C-Glass Fiber, Generic
D-Glass Fiber, Generic
S-Glass Fiber, Generic
S-2 Glass® Fiber

CGF001 / 897

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.