MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

AK Steel 305 Austenitic Stainless steel
Categories: Metal; Ferrous Metal; Austenitic; Stainless Steel; T 300 Series Stainless Steel

Material Notes: AK Steel 305 can be spun and deep drawn more easily due to an increased nickel content that decreases work hardening. It is non-magnetic and cannot be hardened by heat treatment. Typical uses include appliances, kitchen utensils, tank covers and other deep drawn parts.

Information provided by AK Steel

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.99 g/cc0.289 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 8080Annealed
Tensile Strength, Ultimate 586 MPa85000 psiAnnealed
Tensile Strength, Yield 262 MPa
@Strain 0.2 %
38000 psi
@Strain 0.2 %
Annealed
Elongation at Break 50 %50 %in 2 inches, Annealed
Modulus of Elasticity 193 GPa28000 ksi
Izod Impact 140 J103 ft-lbV-Notch (Annealed)
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000720 ohm-cm0.0000720 ohm-cm
Magnetic Permeability <= 1.02<= 1.02H = 200 Oersted, Annealed
 
Thermal PropertiesMetricEnglishComments
CTE, linear  17.3 µm/m-°C
@Temperature 0.000 - 100 °C
9.61 µin/in-°F
@Temperature 32.0 - 212 °F
 18.7 µm/m-°C
@Temperature <=649 °C
10.4 µin/in-°F
@Temperature <=1200 °F
Specific Heat Capacity 0.500 J/g-°C
@Temperature 0.000 - 100 °C
0.120 BTU/lb-°F
@Temperature 32.0 - 212 °F
Thermal Conductivity  16.2 W/m-K
@Temperature 100 °C
112 BTU-in/hr-ft²-°F
@Temperature 212 °F
 21.4 W/m-K
@Temperature 500 °C
149 BTU-in/hr-ft²-°F
@Temperature 932 °F
Melting Point 1399 - 1454 °C2550 - 2649 °F
Solidus 1399 °C2550 °F
Liquidus 1454 °C2649 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.12 %<= 0.12 %
Chromium, Cr 17 - 19 %17 - 19 %
Iron, Fe 64.085 - 73 %64.085 - 73 %As Remainder
Manganese, Mn <= 2.0 %<= 2.0 %
Nickel, Ni 10 - 13 %10 - 13 %
Phosphorus, P <= 0.045 %<= 0.045 %
Silicon, Si <= 1.0 %<= 1.0 %
Sulfur, S <= 0.030 %<= 0.030 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
304 Stainless Steel
AK Steel 316 Austenitic Stainless steel
AK Steel 321 Austenitic Stainless steel
305 Stainless Steel, annealed, sheet
MetalTek Nitronic® 33 Austenitic Stainless Steel

NAKS109 / 14712

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.