MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Plenco 2482 Phenolic, Granular, Transfer Molded
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Phenolic; Phenolic, Novolac, Woodflour Filled

Material Notes: PLENCO 02482 is a general purpose, organic filled phenolic molding compound offering excellent mechanical strength while maintaining dielectric properties at elevated humidity levels. UL recognized under component file E40654. 02482 is available in black.

Information supplied by Plenco.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.650 g/cc0.0235 lb/in³ASTM D1895
Density 1.42 g/cc0.0513 lb/in³ASTM D792
Water Absorption 0.291 %0.291 %ASTM D570
Linear Mold Shrinkage 0.0057 cm/cm0.0057 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell E 8787ASTM D785
Tensile Strength, Ultimate 59.0 MPa8560 psiASTM D638
Elongation at Break 0.82 %0.82 %ASTM D638
Tensile Modulus 8.50 GPa1230 ksiASTM D638
Flexural Strength 94.0 MPa13600 psiASTM D790
Flexural Modulus 8.10 GPa1170 ksiASTM D790
Compressive Strength 206 MPa29900 psiASTM D695
Izod Impact, Notched 0.184 J/cm0.345 ft-lb/inASTM D256
Charpy Impact, Notched 0.198 J/cm²0.942 ft-lb/in²ASTM D256
Impact 9898J/m Drop Ball Impact; PLENCO
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+12 ohm-cm1.00e+12 ohm-cmASTM D247
Dielectric Constant 5.15.1ASTM D150
Dielectric Strength 11.4 kV/mm290 kV/inShort Time; ASTM D149
Dissipation Factor 0.0530.053ASTM D150
Arc Resistance 132 sec132 secASTM D495
Comparative Tracking Index 175 V175 VASTM D3638
 
Thermal PropertiesMetricEnglishComments
CTE, linear 70.0 µm/m-°C
@Temperature 40.0 - 130 °C
38.9 µin/in-°F
@Temperature 104 - 266 °F
TMA; ASTM E831
Thermal Conductivity 0.400 W/m-K
@Temperature 100 °C
2.78 BTU-in/hr-ft²-°F
@Temperature 212 °F
ASTM E1461
Maximum Service Temperature, Air 206 °C403 °FHeat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 168 °C334 °FASTM D648
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
Oxygen Index 27.2 %27.2 %ASTM D2863
Shrinkage 0.21 %0.21 %72 hr, 120ºC; ASTM D1299

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Plenco 1501 Polyester, Briquette, Transfer Molded
Plenco 1501 Polyester, Pellet, Injection Molded
Plenco 1510 Polyester, Granular, Transfer Molded
Plenco 1508 Polyester, Briquette, Transfer Molded
Plenco 1508 Polyester, Briquette, Injection Molded

PLEL47 / 50615

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.