MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

TIMCAL ENSACO™ 260G Conductive Carbon Black
Categories: Carbon; Carbon Black; Other Engineering Material; Additive/Filler for Polymer

Material Notes: ENSACO™ & SUPER P™ conductive carbon blacks possess a high to very high void volume allowing the retention of a carbon network at low to very low filler content. The void volume can originate from the interstices between the carbon black particle due to their complex arrangement and from the porosity.

Applications:

  • black pigment
  • UV stabilizer
  • rubber reinforcement

Information provided by TIMCAL

Key Words: CAS Number 1333-86-4
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.170 g/cc0.00614 lb/in³Pour Density; ASTM D1513
Volatiles <= 0.20 %<= 0.20 %Weight loss during heating between 105 and 950°C; Internal Method 02
Oil Absorption 190 %190 %OAN (Oil Absorption Number) ml/100g; ASTM D2414
Particle Size 45 µm45 µm2 ppm sieve residue; ASTM D1514
pH 8.0 - 118.0 - 11ASTM D1512
Specific Surface Area 70 m²/g70 m²/gBET Nitrogen Surface Area; ASTM D3037
Ash 0.010 %0.010 %ASTM D1506
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 8.0 ohm-cm8.0 ohm-cm25% Carbon Black
 100 ohm-cm100 ohm-cm18% Carbon Black
 1000 ohm-cm1000 ohm-cm15% Carbon Black
 10000 ohm-cm10000 ohm-cm14% Carbon Black
 3.25 ohm-cm
@Time 300 sec
3.25 ohm-cm
@Time 0.0833 hour
25% Carbon Black
 3.5 ohm-cm
@Time 420 sec
3.5 ohm-cm
@Time 0.117 hour
25% Carbon Black
 4.0 ohm-cm
@Time 540 sec
4.0 ohm-cm
@Time 0.150 hour
25% Carbon Black
 50 ohm-cm
@Time 300 sec
50 ohm-cm
@Time 0.0833 hour
18% Carbon Black
 75 ohm-cm
@Time 540 sec
75 ohm-cm
@Time 0.150 hour
18% Carbon Black
 
Component Elements PropertiesMetricEnglishComments
H2O, Water 0.10 %0.10 %as packed; ASTM D1509
Sulfur, S 0.020 %0.020 %ASTM D1619
 
Descriptive Properties
AspectFine black granules
COAN (Crushed OAN) ml/100g104ASTM D3493
Toluene Extract, Max, %0.1ASTM D4527

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
TIMCAL ENSACO™ 250G Conductive Carbon Black Compounds
TIMCAL ENSACO™ 350G Conductive Carbon Black
Graphite, Carbon, C
TIMCAL ENSACO™ 150G Conductive Carbon Black
TIMCAL ENSACO™ 210G Conductive Carbon Black

CTIMCAL03 / 2645

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.