MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Versalis Clearflex® H&T LFH 238 Octene Copolymer Linear Low Density Polyethylene  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade; LLDPE/Octene, Film

Material Notes: Clearflex H&T LFH 238 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidants and processing aid, suitable for blown film extrusion. It contains slip and antiblocking agents.

Films obtained from Clearflex H&T LFH 238 have excellent optical properties (haze and gloss), wide sealing temperature window, together with optimal sealing resistance, outstanding tear, impact and puncture resistance. Its properties make Clearflex H&T LFH 238 the right choice for top end performance applications.

Main Applications: Due to its excellent sealing properties, Clearflex H&T LFH 238 is recommended for packaging food and edible fats and for applications requiring a superior sealing performance. Its very low gel content makes it ideal for lamination.

Information provided by Polimeri Europa.

Versalis is the Eni subsidiary containing the plastics and rubber businesses.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.920 g/cc0.920 g/ccISO 1183
Thickness 10.0 - 50.0 microns0.394 - 1.97 milRecommended
Melt Flow 0.75 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.75 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 10.0 MPa1450 psiISO 527-3
Film Tensile Strength at Yield, TD 10.0 MPa1450 psiISO 527-3
Film Elongation at Break, MD 600 %600 %ISO 527-3
Film Elongation at Break, TD 750 %750 %ISO 527-3
Coefficient of Friction, Dynamic 0.120.12ISO 8295
Elmendorf Tear Strength, MD 18.342 g/micron465.89 g/milISO 6383-2
Elmendorf Tear Strength, TD 25.475 g/micron647.07 g/milISO 6383-2
Dart Drop Test 250 g0.551 lbF50; ISO 7765-1
Film Tensile Strength at Break, MD 50.0 MPa7250 psiISO 527-3
Film Tensile Strength at Break, TD 45.0 MPa6530 psiISO 527-3
1% Secant Modulus, MD 200 MPa29000 psiISO 527-3
1% Secant Modulus, TD 250 MPa36300 psiISO 527-3
 
Thermal PropertiesMetricEnglishComments
Melting Point 119 °C246 °FInternal method
Vicat Softening Point 102 °C
@Load 1.00 kg
216 °F
@Load 2.20 lb
ISO 306/A
Brittleness Temperature <= -70.0 °C<= -94.0 °FASTM D746
 
Optical PropertiesMetricEnglishComments
Haze 11 %11 %ISO 14782
Gloss 60 %60 %45°; ASTM D2457
Transmission, Visible 90 %90 %clear; thickness not quantified

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Braskem LL5800N LLDPE Blown Film Extrusion Polyethylene Copolymer
ExxonMobil C6LL 1017.32 Cast Linear Low Density Polyethylene Resin
Braskem LL6800N LLDPE Blown Film Extrusion Polyethylene Copolymer
Braskem LL5801N LLDPE Blown Film Extrusion Polyethylene Copolymer
Braskem LL4800N PEBDL Cast Film Extrusion Polyethylene Copolymer

PENG076 / 124470

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.