MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Daikin DEMNUM™ S-65 Perfluoropolyether oil
Categories: Fluid; Lubricant; Perfluoropolyether (PFPE)

Material Notes: DEMNUM™ is a perfluoropolyether oil that has a straight-chain structure developed using DAIKIN’s original technology. It has excellent thermal and chemical stability and inertness, and is suitable as a lubricant grease especially when durability and cleanliness are required. DEMNUM GREASE is a grease formed with DEMNUM as the base oil, chemically inert with excellent high-thermal stability and solvent resistance.

Information provided by Daikin.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.873 g/cc1.873 g/cc
Viscosity Measurement 180180Index
Kinematic Viscosity  33 cSt
@Temperature 60.0 °C
33 cSt
@Temperature 140 °F
 150 cSt
@Temperature 20.0 °C
150 cSt
@Temperature 68.0 °F
Kinematic Viscosity at 40°C (104°F) 65 cSt
@Temperature 40.0 °C
65 cSt
@Temperature 104 °F
Kinematic Viscosity at 100°C (212°F) 15 cSt
@Temperature 100 °C
15 cSt
@Temperature 212 °F
Molecular Weight 4500 g/mol4500 g/mol
Vapor Pressure  3.00e-10 bar
@Temperature 20.0 °C
2.25e-7 torr
@Temperature 68.0 °F
 3.00e-7 bar
@Temperature 100 °C
0.000225 torr
@Temperature 212 °F
Surface Tension 18 dynes/cm18 dynes/cm
 
Electrical PropertiesMetricEnglishComments
Dielectric Breakdown 72000 V
@Thickness 2.50 mm
72000 V
@Thickness 0.0984 in
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 1.00 J/g-°C0.239 BTU/lb-°F
Pour Point -65.0 °C-85.0 °F
Glass Transition Temp, Tg -111 °C-168 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.2951.295nD

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Daikin DEMNUM™ S-200 Perfluoropolyether oil
RTP Company RTP 2299 X 113763 B Polyetheretherketone (PEEK), Carbon Fiber - Aramid Fiber - PTFE Lubricated - Perfluoropolyether Oil
Daikin DEMNUM™ S-20 Perfluoropolyether oil
RTP Company RTP 899 X 90822 Acetal (POM), PTFE Lubricated - Perfluoropolyether Oil
RTP Company RTP 399 X 96252 Polycarbonate (PC), Glass Fiber - PTFE Lubricated - Perfluoropolyether Oil

PDAIJ9939 / 210010

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.